Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.570 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2SiO3 + Cr2O3 + Cr |
Band Gap2.630 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPca21 [29] |
HallP 2c 2ac |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 1 0> | 152.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 152.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 94.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 221.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 228.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 144.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 228.0 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 228.0 |
MoS2 (mp-1434) | <1 1 1> | <0 1 0> | 228.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 281.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 55.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 276.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 276.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 55.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 55.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 152.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 165.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 144.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 228.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 165.8 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 165.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 331.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 55.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 154.3 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 76.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 94.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 276.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 144.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 1> | 94.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 221.0 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 228.0 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 228.0 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 331.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 331.5 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 165.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 221.0 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 154.3 |
BN (mp-984) | <1 0 0> | <1 0 1> | 154.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 165.8 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 165.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 94.0 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 276.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 110.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 276.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 221.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 221.0 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 1> | 172.0 |
SiC (mp-7631) | <1 1 1> | <0 0 1> | 165.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 276.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 144.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li10Ti4O13 (mp-772260) | 0.4418 | 0.070 | 3 |
ZnSnO2 (mvc-14586) | 0.5107 | 0.100 | 3 |
Cd4GeS6 (mp-5151) | 0.5848 | 0.012 | 3 |
Cd4GeSe6 (mp-18163) | 0.5757 | 0.018 | 3 |
Si(Hg2Se3)2 (mp-18230) | 0.5440 | 0.017 | 3 |
Li3Fe2(SiO4)2 (mp-763781) | 0.4462 | 0.063 | 4 |
LiSiBiO4 (mp-756818) | 0.4996 | 0.063 | 4 |
LiMnPO4 (mp-765846) | 0.5038 | 0.087 | 4 |
In2Cu2SiS6 (mp-558055) | 0.4602 | 0.055 | 4 |
LiFePO4 (mp-772472) | 0.4990 | 0.426 | 4 |
Cr3N4 (mp-1015065) | 0.7362 | 0.387 | 2 |
Sr2AlCr2GaO7 (mvc-312) | 0.7459 | 0.186 | 5 |
Li2PWO4F (mp-25728) | 0.4894 | 0.352 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Si O |
Final Energy/Atom-6.8034 eV |
Corrected Energy-473.9977 eV
-473.9977 eV = -435.4204 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 16.1040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)