Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.021 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiTi2(PO4)3 |
Band Gap2.489 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 301.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 75.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 129.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 301.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 150.0 |
LiF (mp-1138) | <1 0 0> | <1 1 -1> | 150.0 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 259.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 105.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 301.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 75.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 105.7 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 129.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.4 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 129.9 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 211.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 226.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 211.4 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 301.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 75.5 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 0> | 105.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 301.8 |
PbS (mp-21276) | <1 1 1> | <1 1 0> | 129.9 |
GaP (mp-2490) | <1 0 0> | <1 1 -1> | 150.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 150.9 |
C (mp-66) | <1 1 1> | <1 0 0> | 226.4 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 105.7 |
PbSe (mp-2201) | <1 1 1> | <1 1 0> | 129.9 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 150.9 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 261.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 259.8 |
MoSe2 (mp-1634) | <1 1 0> | <1 1 0> | 259.8 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 261.0 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 105.7 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 211.4 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 301.8 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 105.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 75.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 211.4 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 150.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 301.8 |
Si (mp-149) | <1 0 0> | <1 1 -1> | 150.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 301.8 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 75.5 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 105.7 |
CdSe (mp-2691) | <1 1 1> | <1 1 0> | 129.9 |
C (mp-48) | <0 0 1> | <0 1 0> | 105.7 |
WSe2 (mp-1821) | <1 1 1> | <1 1 0> | 259.8 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 301.8 |
WSe2 (mp-1821) | <0 0 1> | <1 1 0> | 259.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiFeF4 (mp-777472) | 0.4202 | 0.092 | 3 |
MgCrO4 (mp-540704) | 0.4741 | 0.902 | 3 |
FeMoO4 (mp-541843) | 0.4225 | 0.399 | 3 |
MgMoO4 (mp-19047) | 0.4206 | 0.000 | 3 |
MnMoO4 (mp-19081) | 0.4236 | 0.000 | 3 |
LiV2(PO4)3 (mp-540147) | 0.1920 | 0.084 | 4 |
LiCr2(PO4)3 (mp-31688) | 0.2493 | 0.079 | 4 |
LiMo2(PO4)3 (mp-32104) | 0.2563 | 0.001 | 4 |
LiNb2(PO4)3 (mp-26591) | 0.2388 | 0.068 | 4 |
LiCr2(PO4)3 (mp-31667) | 0.2288 | 0.031 | 4 |
Li3Ti3Fe(PO4)6 (mp-743603) | 0.3671 | 0.026 | 5 |
Li9Nb10Cr6(PO4)24 (mp-851292) | 0.2906 | 0.031 | 5 |
Li2Zr7Fe(PO4)12 (mp-774285) | 0.3544 | 0.063 | 5 |
Li3Ti3Fe(PO4)6 (mp-743728) | 0.3865 | 0.013 | 5 |
LiNbSn3(PO4)6 (mp-759486) | 0.3793 | 0.017 | 5 |
Li2Ti2MnCr2(PO4)6 (mp-743387) | 0.5215 | 0.023 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.4436 | 0.114 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4607 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.5198 | 0.011 | 6 |
NaLi3Ti2Al2(PO4)6 (mp-776523) | 0.4575 | 0.036 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv P O |
Final Energy/Atom-7.7366 eV |
Corrected Energy-295.3729 eV
-295.3729 eV = -278.5179 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)