Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.277 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + P + C |
Band Gap4.174 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 49.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 148.3 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 247.2 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 247.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 346.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 247.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 117.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 127.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 346.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 296.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 117.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 117.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 247.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 148.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 346.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 247.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 127.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 296.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 197.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 148.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 346.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 247.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 98.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 346.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 234.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 296.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 148.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 296.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 247.2 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 247.2 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 148.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 346.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 247.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 49.4 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 247.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 296.6 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 234.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 346.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 148.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 98.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 247.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 247.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 296.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 49.4 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 234.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 234.1 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 117.1 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 247.2 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 346.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SiH3I (mp-28538) | 0.5476 | 0.000 | 3 |
AsCF3 (mp-27274) | 0.5096 | 0.494 | 3 |
H3CBr (mp-1078197) | 0.5714 | 0.058 | 3 |
PCF3 (mp-556383) | 0.3920 | 0.600 | 3 |
Si3PH9 (mp-28842) | 0.4100 | 0.000 | 3 |
H9PbC3I (mp-760193) | 0.5899 | 0.207 | 4 |
BPH9C2 (mp-758984) | 0.5481 | 0.072 | 4 |
H8C2BrN (mp-568157) | 0.5969 | 0.049 | 4 |
H8C2NCl (mp-570388) | 0.5746 | 0.047 | 4 |
H9C4Se2N (mp-568817) | 0.5985 | 0.191 | 4 |
NCl3 (mp-540572) | 0.7090 | 0.000 | 2 |
SbH12C4NF4 (mp-600218) | 0.7228 | 0.168 | 5 |
InSi2As(H3C)8 (mp-568872) | 0.6609 | 0.073 | 5 |
H3CSClO (mp-644221) | 0.5014 | 0.245 | 5 |
ZnSi4As2(H3C)12 (mp-570146) | 0.6894 | 0.044 | 5 |
InSi2P(H3C)8 (mp-569070) | 0.7022 | 0.066 | 5 |
H3CSN(ClO)2 (mp-558736) | 0.6218 | 0.457 | 6 |
NaH12C4S2BrO2 (mp-555975) | 0.5419 | 0.138 | 6 |
AlSiH9C3Cl2O (mp-24308) | 0.6603 | 0.000 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: P H C |
Final Energy/Atom-5.0649 eV |
Corrected Energy-526.7497 eV
-526.7497 eV = -526.7497 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)