Final Magnetic Moment4.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.675 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.146 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(CoO2)2 + Li2CO3 + CO2 + CoCO3 |
Band Gap0.338 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 299.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 281.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 299.6 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 222.7 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 222.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 218.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 306.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 59.9 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 299.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 299.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 179.8 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 101.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 59.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 273.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 93.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 122.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 179.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 262.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 122.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 299.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 299.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 262.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 299.6 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 202.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 273.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 299.6 |
BN (mp-984) | <0 0 1> | <1 0 1> | 245.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 175.1 |
BN (mp-984) | <1 0 1> | <0 1 0> | 218.9 |
BN (mp-984) | <1 1 1> | <0 1 0> | 175.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 262.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 281.2 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 119.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 299.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 218.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 131.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 175.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 91.3 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 306.5 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 273.9 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 299.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 299.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 299.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 239.7 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 306.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 179.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 262.7 |
Ni (mp-23) | <1 0 0> | <1 0 1> | 122.8 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 306.5 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 350.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4B2O5 (mp-768884) | 0.7258 | 0.050 | 3 |
Cu(NO3)2 (mp-662543) | 0.7241 | 0.000 | 3 |
LiAg(CO2)2 (mp-985571) | 0.7457 | 0.171 | 4 |
Li3Fe2(CO3)4 (mp-762182) | 0.7279 | 0.269 | 4 |
Li2Fe(CO3)2 (mp-762005) | 0.7292 | 0.240 | 4 |
LiFe2C2O7 (mp-763615) | 0.7188 | 0.127 | 4 |
CuH16C4(N5O)2 (mp-759393) | 0.6563 | 0.045 | 5 |
BaCu2Te2(ClO3)2 (mp-554401) | 0.7029 | 0.009 | 5 |
Li2CuH14C4(N3O4)2 (mp-769075) | 0.6872 | 0.096 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co C O |
Final Energy/Atom-6.7821 eV |
Corrected Energy-147.8181 eV
-147.8181 eV = -135.6426 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)