Final Magnetic Moment10.985 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.149 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi19Ni23O42 + Li(NiO2)2 + NiO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 1 0> | 125.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 251.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 108.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 251.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 251.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 174.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 251.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 167.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 108.2 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 254.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 251.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 174.0 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 197.6 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 254.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 216.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 216.4 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 216.4 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 197.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 216.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 216.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 108.2 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 254.8 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 251.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 174.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 216.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 187.5 |
C (mp-66) | <1 0 0> | <1 0 -1> | 254.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 108.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 167.7 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 251.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 216.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 251.5 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 251.5 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 254.8 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 251.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 251.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 197.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 174.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 143.2 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 251.5 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 251.5 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 251.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 167.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 281.2 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 83.8 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 108.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 216.4 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 167.7 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 187.5 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 108.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3(NiO2)5 (mp-762165) | 0.2274 | 0.041 | 3 |
Li9Co15O28 (mp-762878) | 0.2339 | 0.064 | 3 |
Li3V5O10 (mp-767752) | 0.2631 | 0.207 | 3 |
Li9Ni15O28 (mp-997538) | 0.1487 | 0.033 | 3 |
Li12Ni11O28 (mp-763296) | 0.2446 | 0.043 | 3 |
Li4Mn3(NiO4)3 (mp-762625) | 0.2225 | 0.035 | 4 |
Li6MnNi7O16 (mp-762749) | 0.2001 | 0.196 | 4 |
Li4Ti3(FeO4)3 (mp-762695) | 0.1959 | 0.165 | 4 |
Li4Co3(NiO4)3 (mp-778575) | 0.1991 | 0.019 | 4 |
Li4Cr3(CoO4)3 (mp-763111) | 0.2194 | 0.034 | 4 |
Yb29S30 (mp-685187) | 0.4786 | 0.190 | 2 |
Ni3O4 (mp-714961) | 0.4433 | 0.000 | 2 |
Ni3O4 (mp-656887) | 0.4307 | 0.000 | 2 |
Zr3S4 (mp-684749) | 0.4897 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.5065 | 0.130 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O |
Final Energy/Atom-4.8366 eV |
Corrected Energy-257.7994 eV
-257.7994 eV = -212.8125 eV (uncorrected energy) - 28.1320 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)