Final Magnetic Moment10.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.075 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn3Al2(HO2)6 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 -1 0> | 254.7 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 312.1 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 263.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 181.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 87.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 307.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 323.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 263.5 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 -1> | 279.6 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 169.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 277.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 230.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 277.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 249.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 318.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 238.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 138.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 230.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 138.5 |
KCl (mp-23193) | <1 0 0> | <1 -1 -1> | 279.6 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 169.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 -1 0> | 254.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 230.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 307.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 307.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 230.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 263.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 210.1 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 169.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 138.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 263.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 242.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 230.5 |
TeO2 (mp-2125) | <0 1 1> | <0 1 -1> | 312.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 230.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 159.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 318.4 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 263.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 303.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 -1 0> | 254.7 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 -1> | 312.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 277.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 307.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 92.3 |
MgO (mp-1265) | <1 1 0> | <1 -1 -1> | 279.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 92.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 238.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 230.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeHO2 (mp-626102) | 0.5186 | 0.011 | 3 |
CrHO2 (mp-691133) | 0.5925 | 0.001 | 3 |
CuHO2 (mp-996999) | 0.5305 | 0.047 | 3 |
ScHO2 (mp-625150) | 0.5037 | 0.000 | 3 |
CrHO2 (mp-24927) | 0.5994 | 0.000 | 3 |
Na3Np(HO3)2 (mp-864664) | 0.6135 | 0.037 | 4 |
UHg4(AsCl3)2 (mp-570252) | 0.7365 | 0.000 | 4 |
LiMn3Al2(HO2)6 (mp-762526) | 0.1124 | 0.023 | 5 |
LiMn3Al2(HO2)6 (mp-762521) | 0.1508 | 0.021 | 5 |
LiMn3Al2(HO2)6 (mp-762489) | 0.0936 | 0.023 | 5 |
LiMn3Al2(HO2)6 (mp-762476) | 0.1012 | 0.022 | 5 |
LiMn3Al2(HO2)6 (mp-762475) | 0.1128 | 0.024 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Al H O |
Final Energy/Atom-6.3280 eV |
Corrected Energy-330.6824 eV
-330.6824 eV = -303.7423 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)