Final Magnetic Moment23.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.914 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNiO + Mn3O4 + Li2MnO3 |
Band Gap0.632 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 300.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 250.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 250.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 323.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 250.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 300.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 273.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 277.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 150.4 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 204.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 87.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 250.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 323.9 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 106.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 323.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 175.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 138.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 263.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 213.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 231.4 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 272.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 138.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 277.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 277.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 323.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 323.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 200.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 250.6 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 272.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 250.6 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 204.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 87.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 231.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 138.8 |
BN (mp-984) | <1 1 1> | <1 1 -1> | 104.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 46.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 150.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 323.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 213.0 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 150.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 323.9 |
Al (mp-134) | <1 1 1> | <0 1 0> | 250.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 200.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 277.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 231.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 92.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Fe7O12 (mp-763675) | 0.1833 | 0.051 | 3 |
Li6V5O12 (mp-765419) | 0.2112 | 0.170 | 3 |
Li7(NiO2)9 (mp-762007) | 0.2043 | 0.018 | 3 |
Li4Ni7O12 (mp-997521) | 0.1631 | 0.060 | 3 |
Li6Fe5O12 (mp-780305) | 0.1595 | 0.212 | 3 |
Li4Ti2V5O12 (mp-763676) | 0.1694 | 0.170 | 4 |
Li4V5(FeO6)2 (mp-850103) | 0.1825 | 0.531 | 4 |
Li4Ti2Fe5O12 (mp-762689) | 0.1807 | 0.429 | 4 |
Li4V2Fe5O12 (mp-762682) | 0.1832 | 0.412 | 4 |
Li4V5Cr2O12 (mp-780923) | 0.1304 | 0.053 | 4 |
Fe10O11 (mp-764330) | 0.2248 | 0.057 | 2 |
Fe21O23 (mp-706875) | 0.2367 | 0.055 | 2 |
Fe23O25 (mp-705553) | 0.2218 | 0.051 | 2 |
Fe10O11 (mp-705555) | 0.2459 | 0.046 | 2 |
Fe10O11 (mp-714908) | 0.2493 | 0.046 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.3642 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Ni_pv O |
Final Energy/Atom-6.4022 eV |
Corrected Energy-336.8225 eV
-336.8225 eV = -294.5031 eV (uncorrected energy) - 25.4645 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)