Final Magnetic Moment11.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.444 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnP2O7 + MnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 163.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 243.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 111.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 -1> | 111.8 |
AlN (mp-661) | <0 0 1> | <1 -1 0> | 287.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 230.6 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 162.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 288.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 57.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 229.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 230.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 288.3 |
BN (mp-984) | <0 0 1> | <1 0 1> | 114.8 |
BN (mp-984) | <1 0 1> | <1 1 0> | 261.2 |
BN (mp-984) | <1 1 0> | <1 1 -1> | 235.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 288.3 |
Al (mp-134) | <1 1 1> | <1 -1 -1> | 111.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 288.3 |
SiC (mp-7631) | <0 0 1> | <1 -1 0> | 191.6 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 228.6 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 230.6 |
TbScO3 (mp-31119) | <1 0 1> | <1 -1 -1> | 111.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 173.0 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 242.1 |
LiTaO3 (mp-3666) | <1 0 1> | <1 -1 1> | 223.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 288.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 288.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 242.1 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 288.3 |
NdGaO3 (mp-3196) | <1 0 1> | <1 -1 -1> | 111.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 288.3 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 261.2 |
SiC (mp-11714) | <0 0 1> | <1 -1 0> | 191.6 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 162.6 |
C (mp-66) | <1 1 0> | <0 1 0> | 161.4 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 288.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 -1 0> | 287.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 228.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 288.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 -1 -1> | 111.8 |
Si (mp-149) | <1 1 0> | <0 0 1> | 288.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 288.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 57.7 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 288.3 |
C (mp-48) | <0 0 1> | <0 1 -1> | 162.5 |
C (mp-48) | <1 0 1> | <1 1 0> | 261.2 |
C (mp-48) | <1 1 0> | <0 0 1> | 230.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 288.3 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 288.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 115.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4759 | 0.023 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.4337 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4586 | 0.028 | 3 |
Ni2P3O10 (mp-25610) | 0.4728 | 0.054 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4711 | 0.038 | 3 |
LiSb(PO4)2 (mp-774064) | 0.3888 | 0.072 | 4 |
VNi3(PO4)4 (mp-775192) | 0.3971 | 0.086 | 4 |
NbCo3(PO4)4 (mp-772014) | 0.4039 | 0.261 | 4 |
Li3Mo2P5O18 (mp-585177) | 0.3988 | 0.057 | 4 |
Co3Sb(PO4)4 (mp-768012) | 0.3850 | 0.094 | 4 |
Li4MnV3(P2O7)4 (mp-774458) | 0.4260 | 0.000 | 5 |
Li2VFe(P2O7)2 (mp-764318) | 0.4244 | 0.000 | 5 |
Li2VFe(P2O7)2 (mp-763862) | 0.4244 | 0.003 | 5 |
Li2VFe(P2O7)2 (mp-763861) | 0.4220 | 0.004 | 5 |
Li2MnV(P2O7)2 (mp-764603) | 0.4246 | 0.018 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6649 | 0.081 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5692 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5515 | 0.330 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6805 | 0.513 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6664 | 0.075 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5414 | 0.002 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7356 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.0775 eV |
Corrected Energy-386.4348 eV
-386.4348 eV = -353.8764 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|