Final Magnetic Moment1.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.444 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.146 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFe(PO3)3 |
Band Gap3.758 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 179.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 264.4 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 179.1 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 93.9 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 187.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 168.9 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 274.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 152.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 281.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 168.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 253.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 264.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 274.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 274.4 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 274.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 253.4 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 144.9 |
CdS (mp-672) | <1 1 0> | <1 -1 1> | 243.1 |
Te2W (mp-22693) | <0 1 0> | <1 -1 0> | 274.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 268.7 |
MgO (mp-1265) | <1 1 0> | <0 1 -1> | 182.7 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 281.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 264.4 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 179.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 176.3 |
TiO2 (mp-2657) | <1 1 1> | <1 1 -1> | 264.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 168.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 -1> | 264.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 253.4 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 -1> | 264.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 -1> | 274.0 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 274.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 253.4 |
BN (mp-984) | <1 0 1> | <0 1 -1> | 182.7 |
BN (mp-984) | <1 1 1> | <1 -1 0> | 274.4 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 152.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 -1> | 274.0 |
LaF3 (mp-905) | <1 0 1> | <0 1 -1> | 274.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 -1> | 274.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 253.4 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 -1> | 264.1 |
TbScO3 (mp-31119) | <1 1 1> | <1 -1 0> | 274.4 |
Ni (mp-23) | <1 0 0> | <0 1 -1> | 182.7 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 168.9 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 -1> | 264.1 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 88.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 264.4 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 84.5 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 264.4 |
NdGaO3 (mp-3196) | <1 1 1> | <1 -1 0> | 274.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(P2O7)2 (mp-504329) | 0.5654 | 0.377 | 3 |
Co3(PO4)4 (mp-31551) | 0.5507 | 0.169 | 3 |
Cu3(P2O7)2 (mp-772942) | 0.5893 | 0.060 | 3 |
AlPO4 (mp-1019514) | 0.6160 | 0.083 | 3 |
AlPO4 (mp-1019512) | 0.6111 | 0.085 | 3 |
LiCr(PO3)3 (mp-31641) | 0.4155 | 0.020 | 4 |
LiCu(PO3)3 (mp-558431) | 0.4639 | 0.019 | 4 |
LiSn(PO3)3 (mp-672976) | 0.4683 | 0.026 | 4 |
LiNi(PO3)3 (mp-761648) | 0.1249 | 0.085 | 4 |
LiMn(PO3)3 (mp-762759) | 0.0794 | 0.230 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.8795 eV |
Corrected Energy-421.4678 eV
-421.4678 eV = -385.2534 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)