Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeP2O7 + FePO4 |
Band Gap1.549 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 277.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 154.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 308.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 240.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 77.0 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 240.6 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 291.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 277.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 97.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 231.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 308.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 77.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 308.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 240.6 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 291.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 154.0 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 194.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 277.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 231.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 184.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 231.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 308.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 -1> | 291.7 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 277.3 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 231.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 150.5 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 291.7 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 231.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 0> | 277.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 308.0 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 184.9 |
Mg (mp-153) | <1 1 0> | <1 0 -1> | 291.7 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 154.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 77.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 154.0 |
PbS (mp-21276) | <1 0 0> | <1 0 -1> | 291.7 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 154.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 308.0 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 308.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 308.0 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 231.0 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 308.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 240.6 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 0> | 277.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 308.0 |
Si (mp-149) | <1 0 0> | <1 0 0> | 154.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 154.0 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 77.0 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 184.9 |
C (mp-48) | <0 0 1> | <1 0 -1> | 194.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2P3O10 (mp-540351) | 0.4616 | 0.116 | 3 |
Cr6P7O24 (mp-504359) | 0.4365 | 0.021 | 3 |
Co2P3O10 (mp-25658) | 0.4606 | 0.123 | 3 |
Cr2P3O10 (mp-31635) | 0.4540 | 0.057 | 3 |
Co3(P2O7)2 (mp-540500) | 0.4132 | 0.122 | 3 |
LiTi2P3O11 (mp-762500) | 0.1245 | 0.126 | 4 |
LiTiP2O7 (mp-758145) | 0.3226 | 0.097 | 4 |
LiCr2P3O11 (mp-31661) | 0.1570 | 0.052 | 4 |
LiMo2P3O11 (mp-32071) | 0.3152 | 0.013 | 4 |
LiV2P3O11 (mp-697785) | 0.1720 | 0.229 | 4 |
CrO2 (mvc-11581) | 0.7354 | 0.166 | 2 |
VO2 (mvc-6918) | 0.7309 | 0.095 | 2 |
LiCrPO4F (mp-770575) | 0.4999 | 0.054 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.5150 | 0.130 | 5 |
Na2ZrNi(P2O7)2 (mp-18984) | 0.5167 | 0.058 | 5 |
Na2ZrCo(P2O7)2 (mp-19187) | 0.5265 | 0.030 | 5 |
Na2ZrCo(P2O7)2 (mp-562673) | 0.5053 | 0.030 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5570 | 0.257 | 6 |
Li4TiFe3Cu2(PO4)6 (mp-778677) | 0.6580 | 0.081 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6637 | 0.331 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6820 | 1.367 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6643 | 0.072 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6044 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.9691 eV |
Corrected Energy-263.3329 eV
-263.3329 eV = -236.9505 eV (uncorrected energy) - 15.4504 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)