Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.418 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Li2TiO3 |
Band Gap1.793 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 0> | 308.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 308.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 231.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 324.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 154.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 270.4 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 117.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 54.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 162.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 270.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 308.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 162.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 140.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 282.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 77.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 162.2 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 140.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 324.4 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 188.5 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 270.4 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 282.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 270.4 |
Te2Mo (mp-602) | <1 1 1> | <1 1 0> | 94.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 270.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 270.4 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 270.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 270.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 270.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 140.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 270.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 308.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 162.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 308.7 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 270.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 231.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 270.4 |
SiC (mp-7631) | <1 1 0> | <1 1 1> | 160.4 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 140.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 216.3 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 231.5 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 234.4 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 94.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 77.2 |
TiO2 (mp-2657) | <1 1 1> | <1 0 -1> | 117.2 |
C (mp-66) | <1 0 0> | <1 1 0> | 282.7 |
C (mp-66) | <1 1 0> | <1 0 0> | 54.1 |
C (mp-66) | <1 1 1> | <1 0 0> | 270.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 324.4 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 216.3 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 308.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2(NiO2)3 (mp-762391) | 0.2399 | 0.039 | 3 |
Li2V3O6 (mp-762271) | 0.2335 | 0.054 | 3 |
Li3V7O12 (mp-762285) | 0.1959 | 0.082 | 3 |
Li7(NiO2)10 (mp-767858) | 0.2500 | 0.032 | 3 |
Li5V5O12 (mp-762939) | 0.2457 | 0.087 | 3 |
Li4Ti3V3O12 (mp-763632) | 0.1246 | 0.065 | 4 |
Li4Cr3(FeO4)3 (mp-780090) | 0.1417 | 1.141 | 4 |
Li2MnCr2O6 (mp-850919) | 0.1028 | 0.056 | 4 |
Li2Cr2FeO6 (mp-782636) | 0.1592 | 0.808 | 4 |
Li2VCr2O6 (mp-850093) | 0.1580 | 0.053 | 4 |
Ni6O7 (mp-767815) | 0.3084 | 0.057 | 2 |
V6C5 (mp-28731) | 0.2451 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.3053 | 0.063 | 2 |
Yb43Se45 (mp-684686) | 0.2991 | 0.196 | 2 |
Nb6C5 (mp-2760) | 0.2771 | 0.000 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4684 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Fe_pv O |
Final Energy/Atom-6.8422 eV |
Corrected Energy-254.8319 eV
-254.8319 eV = -225.7926 eV (uncorrected energy) - 16.3980 eV (MP Advanced Correction) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)