Final Magnetic Moment8.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.256 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2NiO4 + Li2NiO3 + Li(NiO2)2 + LiO8 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/m [10] |
Hall-P 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 361.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 115.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 130.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 158.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 187.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 245.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 303.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 231.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 138.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 288.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 216.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 115.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 245.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 187.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 187.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 43.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 216.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 72.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 208.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 288.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 216.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 138.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 277.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 303.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 208.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 130.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 43.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 158.9 |
BN (mp-984) | <1 0 1> | <0 1 0> | 122.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 130.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 332.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 231.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 138.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 115.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 115.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 28.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 187.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 274.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 274.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 130.0 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 244.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 115.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 115.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 115.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 274.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 115.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 115.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 28.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 288.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(NiO2)2 (mp-762255) | 0.3058 | 0.050 | 3 |
Li5(NiO2)8 (mp-762580) | 0.2894 | 0.039 | 3 |
Li6(NiO2)11 (mp-762450) | 0.2741 | 0.040 | 3 |
Li3(NiO2)5 (mp-762386) | 0.2902 | 0.034 | 3 |
Li9Co15O28 (mp-762878) | 0.3005 | 0.085 | 3 |
Li6Fe9CoO20 (mp-765392) | 0.2573 | 0.067 | 4 |
Li8MgCo13O28 (mp-778042) | 0.2400 | 0.065 | 4 |
Li4Fe3Co5O16 (mp-763071) | 0.2306 | 0.066 | 4 |
Li6CoNi9O20 (mp-775263) | 0.2097 | 0.040 | 4 |
LiCoCuO4 (mp-767935) | 0.2728 | 0.062 | 4 |
Ni3O4 (mp-714961) | 0.3949 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.4028 | 0.466 | 2 |
Fe3O4 (mp-612405) | 0.3897 | 0.175 | 2 |
Ni3O4 (mp-656887) | 0.3828 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.4154 | 0.041 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.0554 eV |
Corrected Energy-218.8179 eV
-218.8179 eV = -181.9941 eV (uncorrected energy) - 22.7780 eV (MP Advanced Correction) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)