Final Magnetic Moment1.184 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.413 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiO8 + Fe2NiO4 + Li(NiO2)2 + Li2NiO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 205.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 297.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 274.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 140.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 308.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 247.7 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 234.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 198.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 171.4 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 234.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 205.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 274.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 346.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 140.3 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 210.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 34.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 49.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 171.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 280.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 120.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 280.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 137.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 171.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 308.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 308.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 140.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 171.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 247.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 346.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 241.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 234.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 171.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 247.7 |
Al (mp-134) | <1 0 0> | <0 1 1> | 241.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 240.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 171.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 274.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 34.3 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 120.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 312.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 171.4 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 60.2 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 156.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 297.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 274.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 171.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 1> | 301.2 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 99.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(NiO2)2 (mp-762255) | 0.1163 | 0.050 | 3 |
MgMn2O4 (mp-1097894) | 0.1953 | 0.072 | 3 |
Ca(MnS2)2 (mvc-16788) | 0.2297 | 0.092 | 3 |
LiCr2O4 (mvc-16816) | 0.2399 | 0.237 | 3 |
MgMn2O4 (mp-1002568) | 0.1971 | 0.072 | 3 |
LiTiFeO4 (mp-762701) | 0.1827 | 0.097 | 4 |
Li2FeCo3O8 (mp-763922) | 0.1727 | 0.095 | 4 |
LiCoNiO4 (mp-763751) | 0.1506 | 0.057 | 4 |
Li2MnFe3O8 (mp-768068) | 0.1832 | 0.090 | 4 |
Li2FeNi3O8 (mp-767989) | 0.1857 | 0.066 | 4 |
Ni3O4 (mp-714961) | 0.2565 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.4266 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.4092 | 0.177 | 2 |
Ni3O4 (mp-656887) | 0.2054 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.3750 | 0.130 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Ni_pv O |
Final Energy/Atom-5.4483 eV |
Corrected Energy-91.6886 eV
-91.6886 eV = -76.2763 eV (uncorrected energy) - 9.7940 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)