Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.570 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap2.902 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 231.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 308.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 192.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 223.2 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 324.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 240.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 133.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 178.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 160.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 270.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 267.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 336.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 336.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 178.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 139.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 178.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 272.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 192.0 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 46.4 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 80.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 240.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 324.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 267.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 185.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 288.1 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 185.4 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 267.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 178.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 336.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 133.9 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 -1> | 324.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 240.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 240.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 -1> | 270.1 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 240.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 192.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 288.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 231.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 288.1 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 231.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 231.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 336.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 192.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 336.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 192.0 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 231.8 |
BN (mp-984) | <1 0 1> | <1 0 1> | 80.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 308.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.11368 | 0.11156 | 0.07780 | 0.00000 | 0.02699 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.15806 | 0.00000 | -0.20347 |
0.83455 | 0.50713 | 0.32959 | 0.00000 | -0.22077 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.06654 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
6.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.66 | 0.00 | 0.20 |
0.00 | 3.50 | 0.00 |
0.20 | 0.00 | 3.52 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.73 | 0.00 | 1.60 |
0.00 | 7.60 | 0.00 |
1.60 | 0.00 | 8.45 |
Polycrystalline dielectric constant
εpoly∞
3.56
|
Polycrystalline dielectric constant
εpoly
7.93
|
Refractive Index n1.89 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Be(GaO2)2 (mp-676950) | 0.5579 | 0.116 | 3 |
Li4P2O7 (mp-554577) | 0.5217 | 0.000 | 3 |
Zn2SiO4 (mp-1020636) | 0.4856 | 0.052 | 3 |
Al4CO4 (mp-13703) | 0.5266 | 0.000 | 3 |
Li4P2O7 (mp-28450) | 0.5036 | 0.000 | 3 |
LiCoSiO4 (mp-763246) | 0.4472 | 0.245 | 4 |
LiCoSiO4 (mp-779192) | 0.4324 | 0.346 | 4 |
LiCoSiO4 (mp-762293) | 0.2025 | 0.283 | 4 |
LiFeSiO4 (mp-762703) | 0.4049 | 0.376 | 4 |
LiCuPO4 (mp-504304) | 0.4457 | 0.043 | 4 |
Al12Si12Ag16S5O48 (mp-677726) | 0.6638 | 0.106 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.6581 | 0.003 | 6 |
C (mp-568410) | 0.7278 | 0.507 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8567 eV |
Corrected Energy-106.0011 eV
Uncorrected energy = -95.9931 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV
Corrected energy = -106.0011 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)