Final Magnetic Moment0.424 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.792 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.223 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi4(Ni5O8)3 + Li(NiO2)2 + Li2TiO3 + NiO |
Band Gap0.212 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 44.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 134.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 329.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 106.3 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 176.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 241.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 263.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 290.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 212.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 313.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 223.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 134.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 338.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 233.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 338.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 96.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 268.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 338.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 313.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 241.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 338.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 268.5 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 329.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 241.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 313.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 134.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 263.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 223.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 313.2 |
BN (mp-984) | <1 0 1> | <0 1 1> | 197.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 134.2 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 271.5 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 264.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 241.7 |
Al (mp-134) | <1 1 1> | <0 1 0> | 338.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 134.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 223.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 131.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 1> | 329.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 271.5 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 329.4 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 329.4 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 338.4 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 193.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 223.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 313.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 176.0 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 263.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 193.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4(FeO2)5 (mp-762455) | 0.1883 | 0.198 | 3 |
Li8Mn2O9 (mp-773635) | 0.2169 | 0.171 | 3 |
Li4Ni7O12 (mp-997521) | 0.1649 | 0.060 | 3 |
Li8Fe2O9 (mp-773577) | 0.2164 | 0.178 | 3 |
Li6Fe5O12 (mp-780305) | 0.1923 | 0.212 | 3 |
Li4Mn2Ni5O12 (mp-762588) | 0.1963 | 0.049 | 4 |
Li4Ti2V5O12 (mp-763676) | 0.2101 | 0.170 | 4 |
Li4Ti2Fe5O12 (mp-762689) | 0.1514 | 0.429 | 4 |
Li4V2Fe5O12 (mp-762682) | 0.2084 | 0.412 | 4 |
Li4Mn2Co5O12 (mp-774397) | 0.1779 | 0.555 | 4 |
Fe10O11 (mp-764330) | 0.2370 | 0.057 | 2 |
Fe8O9 (mp-763787) | 0.2822 | 0.063 | 2 |
Fe9O10 (mp-763441) | 0.2558 | 0.040 | 2 |
Fe21O23 (mp-706875) | 0.2443 | 0.055 | 2 |
Fe23O25 (mp-705553) | 0.2541 | 0.051 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.3943 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Ni_pv O |
Final Energy/Atom-5.8117 eV |
Corrected Energy-305.8314 eV
-305.8314 eV = -267.3365 eV (uncorrected energy) - 21.6400 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)