Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.551 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + Li3PO4 |
Band Gap2.505 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 206.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 68.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 68.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 206.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 68.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 275.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 206.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 206.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 275.5 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 206.6 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 275.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 192.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 275.5 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 68.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 206.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 275.5 |
Si (mp-149) | <1 1 1> | <0 0 1> | 206.6 |
Au (mp-81) | <1 1 1> | <0 0 1> | 206.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 192.5 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 275.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 68.9 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 275.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 68.9 |
SiC (mp-8062) | <1 0 0> | <1 0 1> | 192.5 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 275.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 275.5 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 179.7 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 192.5 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 275.5 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 68.9 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 275.5 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 68.9 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 206.6 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 68.9 |
ZnTe (mp-2176) | <1 0 0> | <1 0 1> | 192.5 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 275.5 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 68.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 206.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 206.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.9 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 192.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni2PO5 (mp-769619) | 0.4799 | 0.042 | 3 |
Mn2PO5 (mp-770540) | 0.4130 | 0.018 | 3 |
Cr4P2O9 (mp-773396) | 0.5290 | 0.230 | 3 |
Na2W2O7 (mp-25800) | 0.4826 | 0.021 | 3 |
Mn4(PO4)3 (mp-32010) | 0.5233 | 0.142 | 3 |
Li3Ti2(PO4)3 (mp-759187) | 0.3818 | 0.105 | 4 |
Li5Mn5(PO4)6 (mp-773716) | 0.3826 | 0.243 | 4 |
Li2Fe3(PO4)3 (mp-773357) | 0.3750 | 0.270 | 4 |
Li3Mn(PO4)2 (mp-762881) | 0.3438 | 0.244 | 4 |
Li3Cr(PO4)2 (mp-774182) | 0.2058 | 0.058 | 4 |
Li5Ti3V2(PO4)6 (mp-850911) | 0.3193 | 0.100 | 5 |
Li4Fe5P6WO24 (mp-775677) | 0.3270 | 0.316 | 5 |
Li8VNi3(PO4)6 (mp-765328) | 0.3031 | 0.067 | 5 |
Li5Ti3Mn2(PO4)6 (mp-777015) | 0.3124 | 0.097 | 5 |
Li4Mn5P6WO24 (mp-771110) | 0.3224 | 0.075 | 5 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.3377 | 0.086 | 6 |
Li4Mn2Fe3P6WO24 (mp-770860) | 0.3221 | 0.174 | 6 |
Li4Cr2Ni3Sn(PO4)6 (mp-778614) | 0.3444 | 0.184 | 6 |
Li4Fe2Ni3Sn(PO4)6 (mp-781476) | 0.3418 | 0.081 | 6 |
Li4Co2Ni3Sn(PO4)6 (mp-776757) | 0.3266 | 0.139 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P O |
Final Energy/Atom-6.5697 eV |
Corrected Energy-300.9818 eV
-300.9818 eV = -275.9279 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.1990 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)