Final Magnetic Moment5.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.571 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Si2O5 + Fe2O3 |
Band Gap3.036 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 -1> | 245.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 141.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 282.8 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 133.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 282.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 245.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 141.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 212.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 282.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 141.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 186.7 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 150.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 212.1 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 133.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 141.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 282.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 141.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 282.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 266.0 |
YVO4 (mp-19133) | <1 1 1> | <1 0 -1> | 245.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 266.0 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 282.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 194.1 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 266.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 266.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 141.4 |
BN (mp-984) | <1 1 0> | <0 1 0> | 133.0 |
BN (mp-984) | <1 1 1> | <0 1 0> | 133.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 245.6 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 212.1 |
SiC (mp-7631) | <1 1 0> | <1 0 -1> | 245.6 |
SiC (mp-7631) | <1 1 1> | <1 0 -1> | 245.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 1> | 150.6 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 212.1 |
C (mp-66) | <1 1 1> | <0 1 0> | 133.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 194.1 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 141.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 282.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 282.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 212.1 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 282.8 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 141.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 212.1 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 212.1 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 133.0 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 141.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 -1> | 122.8 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 141.3 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 0> | 266.0 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 0> | 266.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr2Si5N8 (mp-9710) | 0.6178 | 0.000 | 3 |
Na2Ti2O5 (mp-762058) | 0.6654 | 0.033 | 3 |
SrGa4O7 (mp-18253) | 0.6906 | 0.000 | 3 |
MnB4O7 (mp-566848) | 0.6857 | 0.061 | 3 |
LiB3O5 (mp-1020025) | 0.6898 | 0.046 | 3 |
LiCoSiO4 (mp-762976) | 0.1442 | 0.083 | 4 |
LiCoSiO4 (mp-762974) | 0.1981 | 0.089 | 4 |
LiFeSiO4 (mp-762861) | 0.2110 | 0.050 | 4 |
LiCoPO4 (mp-761974) | 0.2853 | 0.045 | 4 |
LiCoPO4 (mp-585212) | 0.3286 | 0.043 | 4 |
YAl6Si18(N15O)2 (mp-677127) | 0.7061 | 0.092 | 5 |
LaAl2Si5N9O (mp-677482) | 0.6240 | 0.150 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-6.8558 eV |
Corrected Energy-642.3899 eV
-642.3899 eV = -575.8840 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 32.7960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)