Final Magnetic Moment13.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.742 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiO8 + Li2FeCo3O8 + Li2CoO3 + Fe2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 178.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 106.9 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 197.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 241.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 49.3 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 246.7 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 296.0 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 345.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 178.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 320.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 151.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 320.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 151.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 235.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 302.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 213.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 171.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 141.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 320.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 320.8 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 106.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 241.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 98.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 142.6 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 185.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 49.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 345.3 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 246.7 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 246.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 71.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 142.6 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 235.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 60.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 308.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 296.0 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 308.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 197.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 106.9 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 185.1 |
Te2Mo (mp-602) | <1 1 1> | <1 1 0> | 185.1 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 49.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 35.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 120.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 345.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 285.1 |
BN (mp-984) | <1 1 0> | <1 1 0> | 246.8 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 246.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 308.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 148.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(NiO2)2 (mp-762255) | 0.2062 | 0.050 | 3 |
MgMn2O4 (mp-1097894) | 0.2190 | 0.072 | 3 |
Li(CoO2)2 (mp-553952) | 0.1636 | 0.027 | 3 |
Ca(MnS2)2 (mvc-16788) | 0.2045 | 0.092 | 3 |
MgMn2O4 (mp-1002568) | 0.2122 | 0.072 | 3 |
Li2FeCo3O8 (mp-763922) | 0.1600 | 0.095 | 4 |
Li2Cr3CoO8 (mp-763336) | 0.0857 | 0.081 | 4 |
Li2CrCo3O8 (mp-763185) | 0.1442 | 0.053 | 4 |
Li2MnFe3O8 (mp-768068) | 0.1454 | 0.090 | 4 |
Li2Fe3CoO8 (mp-763033) | 0.0676 | 0.070 | 4 |
Ni3O4 (mp-714961) | 0.2949 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.2845 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.3156 | 0.177 | 2 |
Ni3O4 (mp-656887) | 0.2784 | 0.000 | 2 |
Ni3O4 (mp-849536) | 0.3574 | 0.130 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Co O |
Final Energy/Atom-6.0440 eV |
Corrected Energy-100.3076 eV
-100.3076 eV = -84.6163 eV (uncorrected energy) - 10.0730 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)