material

MgB2

ID:

mp-763


Tags: Magnesium boride (1/1) Magensium diboride Mgnesium boride (1/2) High pressure experimental phase Magnesium boride (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.130 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.64 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaAs (mp-2534) <1 1 1> <0 0 1> 0.000 57.3
Si (mp-149) <1 1 1> <0 0 1> 0.000 155.5
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.000 155.5
Cu (mp-30) <1 1 1> <1 0 1> 0.004 68.0
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.006 57.3
BaTiO3 (mp-5986) <1 0 1> <1 0 1> 0.009 163.2
TbScO3 (mp-31119) <1 0 0> <1 1 1> 0.010 184.7
Te2Mo (mp-602) <1 1 0> <1 0 0> 0.014 282.4
Ge (mp-32) <1 1 1> <0 0 1> 0.014 57.3
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.015 54.3
BaF2 (mp-1029) <1 1 1> <1 0 1> 0.017 68.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.020 106.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.021 106.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.021 32.7
Mg (mp-153) <1 1 1> <1 0 0> 0.021 152.1
DyScO3 (mp-31120) <1 0 0> <1 1 1> 0.024 184.7
CsI (mp-614603) <1 1 1> <0 0 1> 0.025 106.4
ZnO (mp-2133) <1 0 0> <1 1 1> 0.030 123.1
Ge3(BiO3)4 (mp-23560) <1 0 0> <1 1 0> 0.030 112.9
C (mp-48) <0 0 1> <1 0 1> 0.033 68.0
KP(HO2)2 (mp-23959) <0 0 1> <1 1 0> 0.033 75.3
GdScO3 (mp-5690) <1 0 0> <1 1 1> 0.034 184.7
SrTiO3 (mp-4651) <1 1 0> <1 1 0> 0.037 188.2
Fe2O3 (mp-24972) <0 0 1> <1 0 1> 0.038 68.0
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.039 54.3
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.039 68.0
GaN (mp-804) <1 1 1> <1 0 0> 0.047 152.1
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.048 76.0
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.048 204.0
CdS (mp-672) <0 0 1> <0 0 1> 0.053 106.4
LiF (mp-1138) <1 1 1> <1 0 1> 0.055 204.0
DyScO3 (mp-31120) <1 1 0> <1 1 0> 0.059 188.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.066 43.5
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.066 217.6
Mg (mp-153) <0 0 1> <0 0 1> 0.067 106.4
GaN (mp-804) <0 0 1> <0 0 1> 0.084 106.4
MoS2 (mp-1434) <1 0 0> <1 0 0> 0.087 271.6
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.093 150.5
Te2W (mp-22693) <0 1 0> <1 0 0> 0.096 54.3
NaCl (mp-22862) <1 1 0> <1 0 0> 0.097 228.1
PbSe (mp-2201) <1 1 1> <1 0 1> 0.099 68.0
Mg (mp-153) <1 0 1> <1 0 0> 0.101 76.0
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.111 68.0
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.112 68.0
TbScO3 (mp-31119) <1 1 0> <1 1 0> 0.113 188.2
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.117 106.4
KP(HO2)2 (mp-23959) <1 0 0> <1 1 0> 0.123 112.9
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.125 54.4
InAs (mp-20305) <1 1 0> <1 0 1> 0.127 54.4
SiC (mp-11714) <0 0 1> <0 0 1> 0.128 8.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
421 64 35 0 0 0
64 421 35 0 0 0
35 35 265 0 0 0
0 0 0 70 0 0
0 0 0 0 70 0
0 0 0 0 0 178
Compliance Tensor Sij (10-12Pa-1)
2.5 -0.3 -0.3 0 0 0
-0.3 2.5 -0.3 0 0 0
-0.3 -0.3 3.9 0 0 0
0 0 0 14.2 0 0
0 0 0 0 14.2 0
0 0 0 0 0 5.6
Shear Modulus GV
129 GPa
Bulk Modulus KV
153 GPa
Shear Modulus GR
107 GPa
Bulk Modulus KR
144 GPa
Shear Modulus GVRH
118 GPa
Bulk Modulus KVRH
148 GPa
Elastic Anisotropy
1.09
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
KZnSb (mp-7438) 0.0995 0.000 3
KCuTe (mp-7436) 0.0670 0.000 3
KCuSe (mp-7435) 0.0915 0.000 3
LiMg9B20 (mp-35040) 0.0577 0.024 3
Li4Mg23B54 (mp-530613) 0.0587 0.040 3
BaGa2 (mp-1219) 0.0551 0.000 2
TmB2 (mp-800) 0.0187 0.000 2
LuB2 (mp-11219) 0.0212 0.000 2
HoB2 (mp-2267) 0.0706 0.000 2
ErB2 (mp-1774) 0.0446 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

In a typical procedure, an appropriate amount of anhydrous CrCl3 (0.025mol), Mg (0.025mol) and MgB2 (0.0125mol) were put into a stainless steel autoclave of 50ml capacity. The autoclave was sealed [...]
The starting material in this work is commercially available MgB2 powder (Alfa Aesar, 325 mesh, <44 micron). At room temperature the precursor powder of 0.25g is pressed into the rectangular pellets [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition MgB2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mg_pv B
Final Energy/Atom
-5.1167 eV
Corrected Energy
-15.3501 eV
-15.3501 eV = -15.3501 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 193379
  • 186389
  • 94257
  • 237010
  • 181869
  • 96704
  • 96705
  • 248441
  • 96906
  • 150598
  • 92831
  • 155349
  • 181870
  • 94256
  • 182537
  • 236951
  • 108064
  • 93925
  • 186763
  • 26675
  • 248442
  • 96703
  • 155347
  • 153657
  • 191393
  • 96706
  • 92832
  • 94255
  • 155348
Submitted by
User remarks:
  • Magnesium boride (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)