Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.973 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnF2 + LiF |
Band Gap2.574 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 1> | <0 0 1> | 192.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 228.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.8 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 228.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 192.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 192.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 192.8 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 228.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 228.4 |
C (mp-48) | <1 0 0> | <1 0 0> | 114.2 |
C (mp-48) | <1 1 0> | <1 1 0> | 197.8 |
ZrO2 (mp-2858) | <1 1 -1> | <1 0 0> | 228.4 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 192.8 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 197.8 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 114.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2CuN2 (mvc-15380) | 0.5171 | 0.183 | 3 |
Zn2FeN2 (mvc-13775) | 0.6151 | 0.183 | 3 |
Mn(ZnN)2 (mvc-13664) | 0.5765 | 0.173 | 3 |
LiFeF3 (mp-777489) | 0.4191 | 0.092 | 3 |
SnMo5O8 (mp-19524) | 0.6207 | 0.231 | 3 |
LiMn2(BO3)2 (mp-780816) | 0.7337 | 0.078 | 4 |
LiMnOF2 (mp-767156) | 0.6100 | 0.067 | 4 |
LiVBO4 (mp-770022) | 0.7095 | 0.063 | 4 |
Bi4O5 (mp-684589) | 0.6171 | 0.150 | 2 |
Al2O3 (mp-754531) | 0.5016 | 0.076 | 2 |
Al2S3 (mp-2654) | 0.7115 | 0.000 | 2 |
Al2O3 (mp-754812) | 0.5350 | 0.053 | 2 |
Pb3N2 (mp-1080196) | 0.6366 | 0.355 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv F |
Final Energy/Atom-5.7037 eV |
Corrected Energy-181.1966 eV
-181.1966 eV = -171.1115 eV (uncorrected energy) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)