Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.622 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + Cr(PO3)3 |
Band Gap3.202 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 248.6 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 276.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 97.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 206.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 276.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 165.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 97.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 97.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 92.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 248.6 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 184.2 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 276.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 97.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 276.3 |
BN (mp-984) | <0 0 1> | <0 1 1> | 141.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 292.1 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 248.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 184.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 97.4 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 92.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 276.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 82.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 92.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 194.7 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 276.3 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 292.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 292.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 292.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 276.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 248.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 92.1 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 165.7 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 194.7 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 184.2 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 206.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 97.4 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 248.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 248.6 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 97.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 248.6 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 165.7 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 248.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 292.1 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 194.7 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 248.6 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 165.7 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 292.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 292.1 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 292.1 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 276.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg(PO3)2 (mp-18620) | 0.2681 | 0.000 | 3 |
Cr2P4O13 (mp-562181) | 0.2587 | 0.011 | 3 |
Co(PO3)2 (mp-547237) | 0.2878 | 0.064 | 3 |
Ni(PO3)2 (mp-19135) | 0.2733 | 0.119 | 3 |
Co(PO3)2 (mp-622109) | 0.2845 | 0.064 | 3 |
LiP4WO12 (mp-763463) | 0.2050 | 0.037 | 4 |
Li3Fe(PO3)8 (mp-31887) | 0.1967 | 0.062 | 4 |
LiFe(PO3)4 (mp-762628) | 0.0820 | 0.141 | 4 |
MgV(PO3)4 (mvc-2239) | 0.2286 | 0.057 | 4 |
LiNb(PO3)4 (mp-26767) | 0.2232 | 0.091 | 4 |
Cr19O48 (mp-850874) | 0.7454 | 0.167 | 2 |
LiMnV(P2O7)2 (mp-764454) | 0.5379 | 0.007 | 5 |
LiVFe(P2O7)2 (mp-767272) | 0.5380 | 0.001 | 5 |
MnVP2(HO5)2 (mp-766980) | 0.5390 | 0.046 | 5 |
LiMnV(PO4)3 (mp-770143) | 0.4631 | 0.104 | 5 |
LiMnV(PO4)3 (mp-770057) | 0.4977 | 0.130 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5260 | 0.257 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6712 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6920 | 0.331 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.7150 | 0.001 | 6 |
CsAlBP2HO9 (mp-542129) | 0.7062 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.1858 eV |
Corrected Energy-279.5706 eV
-279.5706 eV = -258.6897 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)