Final Magnetic Moment11.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.341 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.052 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5Ti6FeO16 + LiCoO2 + Li(CoO2)2 + Fe2O3 + TiO2 |
Band Gap0.161 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 1 1> | 111.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 94.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 232.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 166.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 333.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 333.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 174.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 111.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 284.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 160.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 111.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 166.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 166.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 58.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 166.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 116.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 58.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 277.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 189.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 189.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 58.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 174.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 166.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 174.0 |
BN (mp-984) | <1 1 0> | <0 0 1> | 232.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 111.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 166.7 |
Al (mp-134) | <1 1 0> | <0 0 1> | 116.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 58.0 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 248.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 189.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 160.9 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 290.0 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 80.5 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 222.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 333.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 55.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 333.4 |
C (mp-66) | <1 1 0> | <0 1 0> | 284.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 174.0 |
C (mp-66) | <1 0 0> | <1 0 1> | 241.4 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 160.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 111.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 232.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.1525 | 0.074 | 3 |
Zn(AgO2)2 (mvc-4850) | 0.2088 | 0.135 | 3 |
Li9Mn15O32 (mp-769450) | 0.2117 | 0.006 | 3 |
Mn2NiO4 (mp-690543) | 0.2105 | 0.041 | 3 |
Co2SnO4 (mp-706412) | 0.2005 | 0.019 | 3 |
Li4Ti3Fe5O16 (mp-771498) | 0.0852 | 0.071 | 4 |
Li4Mn3Fe5O16 (mp-772388) | 0.0983 | 0.049 | 4 |
Li4Fe5Co3O16 (mp-773387) | 0.1205 | 0.058 | 4 |
Li4Cr3Fe5O16 (mp-772464) | 0.1231 | 0.899 | 4 |
Li4Mn5Co3O16 (mp-771231) | 0.1298 | 0.039 | 4 |
Fe3O4 (mp-715491) | 0.3289 | 0.015 | 2 |
Fe3O4 (mp-542433) | 0.3098 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.2986 | 0.057 | 2 |
Fe3O4 (mp-715558) | 0.3203 | 0.076 | 2 |
Fe3O4 (mp-715811) | 0.3227 | 0.076 | 2 |
Li4Fe3Co3(NiO8)2 (mp-764308) | 0.1100 | 0.055 | 5 |
Li4Mn3Fe3(NiO8)2 (mp-769561) | 0.1064 | 0.065 | 5 |
Li4Mn3Fe2Co3O16 (mp-775386) | 0.1187 | 0.071 | 5 |
Li4Mn3Fe3(CuO8)2 (mp-767314) | 0.1031 | 0.057 | 5 |
Li4Ti3Fe3(NiO8)2 (mp-851004) | 0.0915 | 0.083 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7303 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7188 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7228 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7260 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7284 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Fe_pv Co O |
Final Energy/Atom-6.8567 eV |
Corrected Energy-214.3109 eV
-214.3109 eV = -191.9862 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 11.0880 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)