Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.623 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.102 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVO2 + LiF |
Band Gap1.007 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 256.8 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 267.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 155.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 111.3 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 306.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 220.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 289.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 333.9 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 220.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 346.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 114.7 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 283.4 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 248.5 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 153.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 111.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 283.4 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 153.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 239.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 251.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 306.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 344.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 153.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 333.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 114.7 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 283.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 344.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 344.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 111.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 248.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 289.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 188.9 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 157.4 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 220.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 155.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 306.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 155.8 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 85.6 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 191.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 200.4 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 267.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 222.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 267.1 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 267.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 248.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 157.4 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 191.2 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 111.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 155.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 267.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 289.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3SbO4 (mp-7404) | 0.5788 | 0.000 | 3 |
Na9Ni7O16 (mp-765674) | 0.5705 | 0.033 | 3 |
Li5Fe3O8 (mp-780216) | 0.5008 | 0.483 | 3 |
Na2PtO3 (mp-38017) | 0.5640 | 0.144 | 3 |
Na4TeO5 (mp-15391) | 0.5744 | 0.000 | 3 |
Li2VO2F (mp-763205) | 0.1655 | 0.112 | 4 |
Li2VO2F (mp-763198) | 0.1158 | 0.099 | 4 |
Li2VO2F (mp-763345) | 0.1953 | 0.106 | 4 |
Li2VO2F (mp-763212) | 0.2273 | 0.299 | 4 |
Li2VO2F (mp-763193) | 0.2350 | 0.204 | 4 |
Te2Au (mp-20123) | 0.6729 | 0.000 | 2 |
Te2Au (mp-571547) | 0.6502 | 0.010 | 2 |
Te3Au2 (mp-645449) | 0.7443 | 0.035 | 2 |
BaO (mp-776658) | 0.7186 | 0.019 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.1445 eV |
Corrected Energy-159.8142 eV
-159.8142 eV = -147.4679 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)