Final Magnetic Moment9.369 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.511 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2B4O7 + LiCrO2 + Li2CrO4 |
Band Gap0.479 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 231.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 162.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 291.2 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 187.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 216.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 216.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 285.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 162.0 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 291.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 324.0 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 301.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 270.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 231.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 287.3 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 301.4 |
CdS (mp-672) | <1 1 0> | <1 1 -1> | 242.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 231.2 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 287.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 231.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 270.0 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 291.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 342.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 270.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 301.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 270.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 285.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 162.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 231.2 |
BN (mp-984) | <1 1 1> | <0 1 1> | 301.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 270.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 231.2 |
Al (mp-134) | <1 1 1> | <1 1 0> | 287.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 270.0 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 180.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 171.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 285.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 270.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 180.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 270.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 216.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 54.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 162.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 231.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 270.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 301.4 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 180.9 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 280.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 270.0 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 60.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 77.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Fe(BO3)2 (mp-778811) | 0.6078 | 0.080 | 4 |
CoCu2(BO3)2 (mp-620325) | 0.5157 | 0.147 | 4 |
Li9Cr4(BO3)8 (mp-765270) | 0.1436 | 0.075 | 4 |
MgTi(GeO3)2 (mvc-8038) | 0.6137 | 0.063 | 4 |
Ti2Cu9(B3O11)2 (mp-554562) | 0.5502 | 0.039 | 4 |
Li2AlPCO7 (mp-767214) | 0.6377 | 0.029 | 5 |
Li2FeBPO7 (mp-778767) | 0.6311 | 0.370 | 5 |
Li2FePCO7 (mp-769693) | 0.6025 | 0.172 | 5 |
Li2FePCO7 (mp-770054) | 0.6458 | 0.011 | 5 |
Li2FePCO7 (mp-771292) | 0.6264 | 0.012 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv B O |
Final Energy/Atom-7.0238 eV |
Corrected Energy-340.9775 eV
-340.9775 eV = -316.0706 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)