Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.514 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoHO2 + CO2 + H2O + Li2CO3 |
Band Gap0.692 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 216.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 206.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 170.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 252.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 284.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 254.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 252.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 56.8 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 254.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 170.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 284.0 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 216.4 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 127.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 170.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 127.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 340.8 |
Al (mp-134) | <1 1 0> | <1 0 1> | 254.0 |
Al (mp-134) | <1 1 1> | <0 1 0> | 252.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 252.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 170.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 138.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 227.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 227.2 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 127.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 227.2 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 227.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 340.8 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 206.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 284.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 284.0 |
TiO2 (mp-2657) | <1 0 0> | <1 1 -1> | 166.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 284.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 216.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 284.0 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 170.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 284.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 284.0 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 138.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 170.4 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 227.2 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 127.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 170.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 284.0 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 227.2 |
SiC (mp-11714) | <1 0 1> | <1 1 0> | 163.0 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 103.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 340.8 |
Au (mp-81) | <1 0 0> | <0 0 1> | 170.4 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 284.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 340.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2(CO3)3 (mp-762590) | 0.7067 | 0.280 | 3 |
MgBHO3 (mp-23748) | 0.5985 | 0.000 | 4 |
ZnH8(NO5)2 (mp-23929) | 0.6259 | 0.000 | 4 |
CuH10(CO4)2 (mp-558144) | 0.5814 | 0.103 | 4 |
NiH12(NO6)2 (mp-744954) | 0.5308 | 0.034 | 4 |
ZnH6(CO3)2 (mp-24313) | 0.6272 | 0.076 | 4 |
Na2CoH8(CO5)2 (mp-735556) | 0.5937 | 0.080 | 5 |
Li2CoH8(CO5)2 (mp-770598) | 0.5536 | 0.073 | 5 |
Na2CuH6C2O9 (mp-24228) | 0.5631 | 0.019 | 5 |
Li2NiH8(CO5)2 (mp-771916) | 0.6053 | 0.080 | 5 |
ZnH16C6(N3O5)2 (mp-698329) | 0.5193 | 0.037 | 5 |
H48PtW6C8(NO)24 (mp-773991) | 0.7118 | 0.068 | 6 |
SiH18C2N8(OF3)2 (mp-766429) | 0.7339 | 0.088 | 6 |
MnH18C4N8(ClO)4 (mp-735514) | 0.5650 | 0.082 | 6 |
VH16C6N6O7F2 (mp-565253) | 0.6638 | 0.132 | 6 |
CoH18C4N8(ClO)4 (mp-744629) | 0.5484 | 0.036 | 6 |
ReH12C2S2N4Cl5O3 (mp-720928) | 0.6157 | 0.102 | 7 |
ReH22C4S4N8Cl8O3 (mp-720895) | 0.6417 | 0.084 | 7 |
Mo3H8C4SN2Cl6O7 (mp-744073) | 0.6912 | 0.169 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co H C O |
Final Energy/Atom-5.7851 eV |
Corrected Energy-272.3401 eV
-272.3401 eV = -254.5463 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)