Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.352 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + SiO2 |
Band Gap1.475 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 212.0 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 206.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 112.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 123.8 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 82.5 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 203.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 218.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 43.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 306.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 65.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 135.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 175.1 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 272.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 140.1 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 181.6 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 135.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 87.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 224.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 212.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 28.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 140.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 195.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 270.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 175.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 65.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 43.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 56.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 43.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 218.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 306.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 151.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 212.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 123.8 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 206.3 |
MoS2 (mp-1434) | <1 1 0> | <1 0 -1> | 236.8 |
MoS2 (mp-1434) | <1 1 1> | <1 0 -1> | 236.8 |
Al (mp-134) | <1 0 0> | <1 0 1> | 65.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 67.7 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 169.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 28.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 165.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 41.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 206.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 135.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 336.2 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 270.6 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 131.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 65.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 67.7 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 224.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Be(GaO2)2 (mp-676950) | 0.3656 | 0.116 | 3 |
Li2CrO4 (mp-769767) | 0.4083 | 0.020 | 3 |
Li2MnF4 (mp-763098) | 0.3892 | 0.093 | 3 |
Zn2SiO4 (mp-1020721) | 0.4083 | 0.111 | 3 |
Zn2SiO4 (mp-1020594) | 0.4014 | 0.010 | 3 |
LiFeSiO4 (mp-861551) | 0.1055 | 0.080 | 4 |
LiCoSiO4 (mp-779191) | 0.1202 | 0.076 | 4 |
LiFeSiO4 (mp-767283) | 0.0612 | 0.072 | 4 |
LiFeSiO4 (mp-762804) | 0.1129 | 0.069 | 4 |
LiCoSiO4 (mp-762722) | 0.0923 | 0.088 | 4 |
Ge3N4 (mp-672289) | 0.5800 | 0.000 | 2 |
Cr3N4 (mp-1014369) | 0.5516 | 0.114 | 2 |
Si3N4 (mp-2245) | 0.5766 | 0.000 | 2 |
CN2 (mp-1077595) | 0.5527 | 0.691 | 2 |
Ti3N4 (mp-1080190) | 0.5287 | 0.119 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.5662 | 0.031 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.5345 | 0.000 | 5 |
Li4Al3Ge3IO12 (mp-557456) | 0.5776 | 0.000 | 5 |
Li4Ga3Si3BrO12 (mp-556649) | 0.5749 | 0.000 | 5 |
Mn4Be3Ge3SO12 (mp-25772) | 0.5961 | 0.000 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5523 | 0.003 | 6 |
C (mp-680372) | 0.6455 | 0.407 | 1 |
C (mp-630227) | 0.7420 | 0.394 | 1 |
C (mp-568028) | 0.7417 | 0.529 | 1 |
C (mp-568410) | 0.5374 | 0.507 | 1 |
C (mp-1008374) | 0.5956 | 0.437 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.5733 eV |
Corrected Energy-101.3927 eV
-101.3927 eV = -92.0264 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)