Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.372 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(CoO2)2 + SiO2 + Li2Si2O5 + Co3O4 |
Band Gap1.373 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 339.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 238.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 79.6 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 194.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 135.7 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 139.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 238.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 -1> | 340.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 345.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 189.6 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 215.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 237.5 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 203.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 318.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 101.8 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 212.3 |
GaSe (mp-1943) | <1 1 0> | <0 1 0> | 237.5 |
GaSe (mp-1943) | <1 1 1> | <0 1 0> | 237.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 132.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 79.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 79.6 |
BN (mp-984) | <1 1 0> | <0 1 1> | 129.2 |
BN (mp-984) | <1 1 1> | <0 1 1> | 129.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 185.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 212.3 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 301.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 165.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 203.6 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 215.4 |
Al (mp-134) | <1 0 0> | <0 1 0> | 271.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 212.3 |
Al (mp-134) | <1 1 1> | <0 1 0> | 203.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 87.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 129.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 43.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 215.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 339.3 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 55.2 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 135.7 |
CdTe (mp-406) | <1 1 0> | <1 1 -1> | 243.0 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 286.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 304.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 1> | 189.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 130.7 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 189.6 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 291.9 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 79.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 238.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 339.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 185.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCoSiO4 (mp-762880) | 0.0936 | 0.060 | 4 |
LiFeSiO4 (mp-762581) | 0.1118 | 0.018 | 4 |
LiFeSiO4 (mp-763641) | 0.1427 | 0.023 | 4 |
LiVSiO4 (mp-767103) | 0.1381 | 0.070 | 4 |
LiFeSiO4 (mp-775228) | 0.0479 | 0.023 | 4 |
Cr3N4 (mp-1014369) | 0.3631 | 0.083 | 2 |
Si3N4 (mp-2245) | 0.4403 | 0.000 | 2 |
Ge3N4 (mp-672289) | 0.4554 | 0.000 | 2 |
C3N4 (mp-9410) | 0.4321 | 0.288 | 2 |
C3N4 (mp-1985) | 0.5659 | 0.325 | 2 |
Li2SO4 (mp-4556) | 0.3822 | 0.000 | 3 |
Zn2SiO4 (mp-1020594) | 0.2255 | 0.010 | 3 |
Li2MnF4 (mp-763098) | 0.3415 | 0.091 | 3 |
Li2CrO4 (mp-769767) | 0.2850 | 0.021 | 3 |
Li2FeF4 (mp-777130) | 0.3372 | 0.090 | 3 |
YAl6Si30(N15O)3 (mp-677140) | 0.5112 | 0.084 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.4967 | 0.000 | 5 |
YAl6Si18(N15O)2 (mp-677127) | 0.5368 | 0.092 | 5 |
Li4Be3P3BrO12 (mp-554560) | 0.5418 | 0.000 | 5 |
Be3Fe4Si3TeO12 (mp-704630) | 0.5011 | 0.000 | 5 |
C (mp-568028) | 0.7281 | 0.529 | 1 |
C (mp-1008374) | 0.6894 | 0.437 | 1 |
C (mp-680372) | 0.6998 | 0.407 | 1 |
C (mp-630227) | 0.7416 | 0.393 | 1 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5578 | 0.002 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points48 |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.5868 eV |
Corrected Energy-101.5811 eV
-101.5811 eV = -92.2148 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)