Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.198 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.246 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + SiO2 |
Band Gap1.396 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 99.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 298.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 166.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 234.2 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 234.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 190.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 33.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 132.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 232.4 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 87.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 133.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 256.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 234.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 313.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 199.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 33.2 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 111.1 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 143.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 132.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 87.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 284.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 166.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 265.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 166.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 199.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 256.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 166.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 234.2 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 234.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 142.3 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 143.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 298.8 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 262.3 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 142.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 166.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 66.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 95.4 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 99.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 132.8 |
YVO4 (mp-19133) | <1 0 1> | <1 1 1> | 277.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 298.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 298.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 234.2 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 190.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 341.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 238.6 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 263.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 365.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 234.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 133.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2SiO4 (mp-3789) | 0.5008 | 0.000 | 3 |
Be(GaO2)2 (mp-676950) | 0.4074 | 0.116 | 3 |
Li2CrO4 (mp-769767) | 0.4911 | 0.020 | 3 |
Zn2SiO4 (mp-1020594) | 0.4912 | 0.010 | 3 |
Li2BeF4 (mp-4622) | 0.4946 | 0.000 | 3 |
LiCoSiO4 (mp-763246) | 0.3277 | 0.104 | 4 |
LiVSiO4 (mp-767068) | 0.3233 | 0.056 | 4 |
LiFeSiO4 (mp-767253) | 0.2751 | 0.034 | 4 |
LiCoSiO4 (mp-763240) | 0.3031 | 0.068 | 4 |
LiFeSiO4 (mp-762639) | 0.2372 | 0.021 | 4 |
CuS2 (mp-684604) | 0.6834 | 0.100 | 2 |
C3N4 (mp-571653) | 0.7192 | 0.484 | 2 |
Cr3N4 (mp-1014369) | 0.7229 | 0.164 | 2 |
SiC2 (mp-1019097) | 0.7095 | 0.562 | 2 |
CN2 (mp-1077595) | 0.6804 | 0.691 | 2 |
Be3Fe4Si3SO12 (mp-627398) | 0.5814 | 0.203 | 5 |
Li4Ga3Si3IO12 (mp-557112) | 0.5566 | 0.000 | 5 |
Li4Ga3Si3ClO12 (mp-554203) | 0.6073 | 0.000 | 5 |
Li4Ga3Si3BrO12 (mp-556649) | 0.5898 | 0.000 | 5 |
Be3Fe4Si3TeO12 (mp-704630) | 0.5840 | 0.168 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5690 | 0.003 | 6 |
C (mp-568410) | 0.6827 | 0.507 | 1 |
C (mp-1008374) | 0.7104 | 0.437 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.4196 eV |
Corrected Energy-99.2401 eV
-99.2401 eV = -89.8738 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)