Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.239 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.165 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoPO4 + LiF |
Band Gap0.394 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 173.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 136.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 288.7 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 268.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 204.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 288.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 115.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 268.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 57.7 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 288.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 57.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 173.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 288.7 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 268.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 272.7 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 268.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 288.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 268.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 288.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 288.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 173.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 268.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 272.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 204.5 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 268.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 268.0 |
BN (mp-984) | <1 0 0> | <0 1 1> | 268.0 |
BN (mp-984) | <1 1 1> | <0 1 1> | 268.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 288.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 288.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 272.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 230.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 136.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 173.2 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 150.3 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 230.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 150.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 288.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 230.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 272.7 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 230.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 204.5 |
C (mp-66) | <1 1 0> | <0 1 1> | 89.3 |
C (mp-66) | <1 1 1> | <0 1 1> | 89.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 115.5 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 57.7 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 230.9 |
Ni (mp-23) | <1 1 0> | <1 1 1> | 175.1 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 173.2 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 204.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-650392) | 0.6162 | 0.821 | 3 |
Na2W2O7 (mp-25800) | 0.6147 | 0.021 | 3 |
MnSiO3 (mp-565815) | 0.6477 | 0.007 | 3 |
MnSiO3 (mp-19528) | 0.6379 | 0.007 | 3 |
MgSiO3 (mp-1020115) | 0.6337 | 0.031 | 3 |
Li3Mn2(PO4)3 (mp-850909) | 0.5759 | 0.057 | 4 |
Li3Mn2(PO4)3 (mp-761591) | 0.5510 | 0.190 | 4 |
Li2Mn3(PO4)4 (mp-762618) | 0.5605 | 0.041 | 4 |
Li2NiP2O7 (mp-779070) | 0.5711 | 0.002 | 4 |
LiVPO5 (mp-772256) | 0.5379 | 0.116 | 4 |
K4Li5Ti8(PO5)8 (mp-766028) | 0.5901 | 0.041 | 5 |
Li3MnV(PO4)3 (mp-779876) | 0.5907 | 0.219 | 5 |
KLiTi2(PO5)2 (mp-774482) | 0.6380 | 0.027 | 5 |
Li3MnV(PO4)3 (mp-779367) | 0.5816 | 0.145 | 5 |
Li2Ti4Co(AsO5)4 (mp-744463) | 0.6143 | 0.072 | 5 |
Li4Mn2CrNi3(PO4)6 (mp-775171) | 0.7242 | 0.085 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.7070 | 0.080 | 6 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.7225 | 0.095 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.6938 | 0.075 | 6 |
Li4TiCo2Ni3(PO4)6 (mp-778251) | 0.7245 | 0.203 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6693 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O F |
Final Energy/Atom-6.1089 eV |
Corrected Energy-428.4355 eV
-428.4355 eV = -390.9702 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 14.9920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)