Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CoSiO4 + Co2SiO4 + SiO2 |
Band Gap2.346 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinAma2 [40] |
HallA 2 2a |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 141.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 124.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 231.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 277.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 231.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 162.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 200.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 248.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 265.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 124.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 267.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 267.7 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 200.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 231.0 |
BN (mp-984) | <1 0 1> | <0 1 1> | 81.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 46.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 323.4 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 81.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 124.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 132.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 277.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 81.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 138.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 277.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 162.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 124.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 244.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 81.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 277.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 138.6 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 231.0 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 162.7 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 323.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 132.6 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 267.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 231.0 |
C (mp-66) | <1 1 0> | <0 1 1> | 162.7 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 231.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 1> | 162.7 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 244.0 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 124.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 277.2 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 323.4 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 277.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 138.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 231.0 |
Au (mp-81) | <1 1 0> | <0 0 1> | 277.2 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 124.3 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 1> | 265.2 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 92.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-762058) | 0.7048 | 0.031 | 3 |
Ag4P2S7 (mp-27482) | 0.7133 | 0.007 | 3 |
Ag7P3S11 (mp-683910) | 0.6480 | 0.019 | 3 |
SrAl2O4 (mp-3094) | 0.6974 | 0.000 | 3 |
Ca5Al6O14 (mp-17694) | 0.6868 | 0.003 | 3 |
Na2Zn2Si2O7 (mp-6507) | 0.4196 | 0.000 | 4 |
Li2Mn2Si2O7 (mp-767364) | 0.2641 | 0.084 | 4 |
Li2Fe2Si2O7 (mp-762576) | 0.4040 | 0.552 | 4 |
Na2Mn2Si2O7 (mp-555689) | 0.4529 | 0.506 | 4 |
Na2Mn2Si2O7 (mp-640448) | 0.4505 | 0.506 | 4 |
Li6CoCu3(PO4)4 (mp-775260) | 0.7301 | 0.099 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co Si O |
Final Energy/Atom-6.6956 eV |
Corrected Energy-190.2553 eV
Uncorrected energy = -174.0853 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -190.2553 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)