Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.546 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.047 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + Li3PO4 + W |
Band Gap3.958 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 296.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 296.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 238.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 63.8 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 178.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 237.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 211.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 175.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 95.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 140.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 159.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 281.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 35.2 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 255.1 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 191.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 59.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 95.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 214.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 140.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 238.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 47.6 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 159.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 281.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 95.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 175.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 281.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 175.9 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 105.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 190.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 159.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 281.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 95.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 140.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 296.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 175.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 319.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 351.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 238.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 265.9 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 296.7 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 255.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 70.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 319.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 175.9 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 191.3 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 265.9 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 191.3 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 318.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 265.9 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 63.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.00000 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.08 | -0.01 | 0.03 |
-0.01 | 3.11 | -0.00 |
0.03 | -0.00 | 2.87 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.43 | -7.26 | 0.01 |
-7.26 | 18.74 | -0.15 |
0.01 | -0.15 | 6.38 |
Polycrystalline dielectric constant
εpoly∞
3.02
|
Polycrystalline dielectric constant
εpoly
12.52
|
Refractive Index n1.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co3(PO4)2 (mp-651271) | 0.4728 | 0.016 | 3 |
VSiO3 (mp-769952) | 0.4489 | 0.019 | 3 |
Li2SO4 (mp-558382) | 0.3268 | 0.055 | 3 |
Na2CrO4 (mp-18779) | 0.4146 | 0.000 | 3 |
Na2FeO4 (mp-19044) | 0.4377 | 0.062 | 3 |
Li3Mo(PO4)2 (mp-32100) | 0.0540 | 0.025 | 4 |
Li3Ti(PO4)2 (mp-757905) | 0.1431 | 0.072 | 4 |
Li3Fe(PO4)2 (mp-31787) | 0.1761 | 0.029 | 4 |
Li3V(PO4)2 (mp-32456) | 0.1715 | 0.027 | 4 |
Li3Ni(PO4)2 (mp-540367) | 0.1724 | 0.060 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.3110 | 0.022 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.2918 | 0.131 | 5 |
Li7Fe7P6(O8F)3 (mp-997551) | 0.3142 | 0.219 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.4487 | 0.077 | 5 |
Li7Cr7P6(O8F)3 (mp-763893) | 0.4383 | 0.031 | 5 |
Li3VCrP2(O4F)2 (mp-766992) | 0.7457 | 0.027 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6237 | 0.008 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.7411 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-6.7695 eV |
Corrected Energy-104.7064 eV
Uncorrected energy = -94.7724 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-4.438 eV/atom x 1.0 atoms) = -4.4380 eV
Corrected energy = -104.7064 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)