Final Magnetic Moment1.013 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.530 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP2WO8 + P3(WO6)2 + LiPO3 + P2O5 |
Band Gap2.537 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 236.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 295.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 141.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 188.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 141.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 141.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 236.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 295.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 137.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 137.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 236.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 177.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 295.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 295.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 177.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 177.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 177.0 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 141.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 236.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 236.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 236.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 177.0 |
LaF3 (mp-905) | <1 0 1> | <0 1 1> | 137.8 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 177.0 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 295.1 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 141.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 295.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 188.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 177.0 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 141.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 295.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 177.0 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 236.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 295.1 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 141.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 141.3 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 295.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 295.1 |
Si (mp-149) | <1 1 0> | <0 0 1> | 295.1 |
Au (mp-81) | <1 1 0> | <0 0 1> | 295.1 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 236.1 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 236.1 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 236.1 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 236.1 |
C (mp-48) | <0 0 1> | <0 0 1> | 236.1 |
C (mp-48) | <1 1 1> | <0 0 1> | 236.1 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 141.3 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 177.0 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 236.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 177.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeP4O11 (mp-746730) | 0.2445 | 0.087 | 3 |
NiP4O11 (mp-764190) | 0.2739 | 0.009 | 3 |
ZnP4O11 (mp-774868) | 0.2393 | 0.006 | 3 |
CoP4O11 (mp-763297) | 0.2672 | 0.126 | 3 |
CrP4O11 (mp-772704) | 0.2770 | 0.131 | 3 |
LiP4WO12 (mp-763455) | 0.3779 | 0.017 | 4 |
LiSb(PO3)4 (mp-504340) | 0.2926 | 0.042 | 4 |
LiMoP4O13 (mp-32076) | 0.2654 | 0.042 | 4 |
LiNb(PO3)4 (mp-757816) | 0.3401 | 0.118 | 4 |
LiSn(PO3)4 (mp-757616) | 0.3123 | 0.078 | 4 |
V5O12 (mp-776915) | 0.5975 | 0.032 | 2 |
MgCr3Se2(SO6)4 (mp-769544) | 0.5822 | 0.126 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.5646 | 0.180 | 5 |
LiBS4(ClO3)4 (mp-555090) | 0.5934 | 0.005 | 5 |
Cs3Mg3In(PO3)12 (mp-720658) | 0.6388 | 0.006 | 5 |
SbPH4(O2F3)2 (mp-973330) | 0.6387 | 0.000 | 5 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.6808 | 0.030 | 6 |
RbScBP2HO9 (mp-23809) | 0.6376 | 0.000 | 6 |
CsAlBP2HO9 (mp-542129) | 0.5621 | 0.000 | 6 |
RbAlBP2HO9 (mp-542130) | 0.6011 | 0.000 | 6 |
CsFeBP2HO9 (mp-761395) | 0.6550 | 0.118 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-7.1276 eV |
Corrected Energy-595.6237 eV
-595.6237 eV = -541.7006 eV (uncorrected energy) - 36.5191 eV (MP Anion Correction) - 17.4040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)