Final Magnetic Moment0.946 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.506 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPWO5 + LiPO3 |
Band Gap3.563 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 1 1> | 161.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 201.0 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 269.2 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 265.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 240.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 80.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 281.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 130.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 160.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 140.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 130.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 130.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 140.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 130.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 160.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 321.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 321.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 160.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 261.0 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 132.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 140.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 321.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 321.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 281.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 201.0 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 201.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 261.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 240.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 321.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 281.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 321.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 240.7 |
BN (mp-984) | <1 0 0> | <1 1 -1> | 155.0 |
BN (mp-984) | <1 0 1> | <1 0 0> | 261.0 |
BN (mp-984) | <1 1 1> | <0 0 1> | 241.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 281.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 201.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 120.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 80.4 |
MoS2 (mp-1434) | <1 0 1> | <0 0 1> | 281.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 265.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 130.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 140.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 321.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 130.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 140.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 80.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 160.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 321.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 132.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2P4O13 (mp-770561) | 0.5201 | 0.005 | 3 |
Hg2P2O7 (mp-28455) | 0.5013 | 0.000 | 3 |
Mo3(PO4)4 (mp-705297) | 0.5140 | 0.046 | 3 |
Cr2P3O10 (mp-31635) | 0.5400 | 0.057 | 3 |
Mn4P7O24 (mp-690039) | 0.4543 | 0.016 | 3 |
LiMn4P7O24 (mp-697807) | 0.4322 | 0.034 | 4 |
LiCoP2O7 (mp-767244) | 0.4416 | 0.032 | 4 |
LiMnP2O7 (mp-762780) | 0.4589 | 0.066 | 4 |
LiMnP2O7 (mp-689993) | 0.4506 | 0.027 | 4 |
LiMn2P3O11 (mp-540021) | 0.4433 | 0.041 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.5800 | 0.087 | 5 |
NaCoP2HO7 (mp-40668) | 0.6440 | 0.001 | 5 |
KBaYSi2O7 (mp-559670) | 0.6380 | 0.000 | 5 |
NaZnFe2(PO4)3 (mp-566178) | 0.4840 | 0.007 | 5 |
NaCoP2HO7 (mp-703256) | 0.6247 | 0.001 | 5 |
NaCoBP2H2O9 (mp-601388) | 0.6528 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-7.1149 eV |
Corrected Energy-381.3915 eV
-381.3915 eV = -341.5142 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 17.4040 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)