Final Magnetic Moment38.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.736 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + Fe2O3 |
Band Gap1.604 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 109.7 |
AlN (mp-661) | <1 0 0> | <1 -1 -1> | 111.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 122.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 282.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 219.8 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 -1> | 124.0 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 224.1 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 81.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 237.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 186.0 |
GaAs (mp-2534) | <1 1 1> | <0 1 -1> | 286.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 282.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 124.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 204.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 -1> | 163.6 |
BaF2 (mp-1029) | <1 1 1> | <0 1 -1> | 204.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 146.3 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 272.7 |
GaAs (mp-2534) | <1 0 0> | <1 -1 0> | 224.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 113.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 219.5 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 230.8 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 278.2 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 170.5 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 292.6 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 204.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 219.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 186.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 204.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 81.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 94.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 323.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 282.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 113.7 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 163.6 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 204.5 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 0> | 224.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 186.0 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 286.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 1> | 161.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 224.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 230.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 -1 0> | 313.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 186.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 170.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 205.8 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 268.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 0> | 224.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 -1> | 204.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Fe7O12 (mp-763675) | 0.1760 | 0.050 | 3 |
Li4V7O12 (mp-762252) | 0.1903 | 0.060 | 3 |
Li4Cr5O10 (mp-763579) | 0.1545 | 0.035 | 3 |
Li3(FeO2)4 (mp-764718) | 0.2414 | 0.097 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.2201 | 0.106 | 3 |
Li4V5O9F (mp-765520) | 0.1703 | 0.066 | 4 |
Li3V2(FeO4)2 (mp-763659) | 0.1752 | 0.088 | 4 |
Li3V2Cr2O8 (mp-850135) | 0.1832 | 0.057 | 4 |
Li4Cr2Fe5O12 (mp-850397) | 0.1781 | 1.110 | 4 |
Li4Cr2Ni5O12 (mp-780901) | 0.1896 | 0.099 | 4 |
Fe11O12 (mp-705417) | 0.1441 | 0.049 | 2 |
Fe8O9 (mp-763787) | 0.1401 | 0.061 | 2 |
Fe8O9 (mp-705588) | 0.1530 | 0.049 | 2 |
Fe21O23 (mp-706875) | 0.1705 | 0.052 | 2 |
Fe10O11 (mp-705555) | 0.1248 | 0.044 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4523 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O |
Final Energy/Atom-6.6882 eV |
Corrected Energy-158.6955 eV
-158.6955 eV = -127.0756 eV (uncorrected energy) - 24.5970 eV (MP Advanced Correction) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)