Final Magnetic Moment2.011 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.510 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + Li3PO4 + W |
Band Gap2.440 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 110.7 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 132.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 132.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 234.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 312.0 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 132.3 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 264.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 234.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 234.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 156.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.0 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 110.7 |
GaP (mp-2490) | <1 0 0> | <1 1 -1> | 153.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 312.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 156.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 156.0 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 312.0 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 264.6 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 221.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 312.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 156.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 78.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 -1> | 110.7 |
PbSe (mp-2201) | <1 1 1> | <0 1 1> | 132.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 234.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 312.0 |
BN (mp-984) | <1 1 0> | <0 1 1> | 132.3 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 -1> | 153.9 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 312.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 1> | 189.9 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 134.4 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 1> | 264.6 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 1> | 264.6 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 -1> | 221.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 -1> | 153.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 312.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 134.4 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 213.7 |
Au (mp-81) | <1 1 0> | <1 0 -1> | 221.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 132.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 78.0 |
CdSe (mp-2691) | <1 1 0> | <1 0 -1> | 110.7 |
CdSe (mp-2691) | <1 1 1> | <0 1 1> | 132.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 156.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 134.4 |
C (mp-48) | <1 1 0> | <0 1 1> | 132.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 312.0 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 134.4 |
WSe2 (mp-1821) | <1 1 0> | <0 1 1> | 264.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3(P2O7)2 (mp-569271) | 0.4553 | 0.001 | 3 |
MnCrO4 (mp-769911) | 0.4530 | 0.073 | 3 |
MgCrO4 (mp-540704) | 0.4463 | 0.902 | 3 |
Cr3(P2O7)2 (mp-774562) | 0.4568 | 0.001 | 3 |
MnMoO4 (mp-19081) | 0.4500 | 0.000 | 3 |
LiSn2(PO4)3 (mp-26702) | 0.2211 | 0.002 | 4 |
LiNi2(SO4)3 (mp-778860) | 0.2247 | 0.067 | 4 |
LiMo2(PO4)3 (mp-32104) | 0.1242 | 0.001 | 4 |
LiNb2(PO4)3 (mp-26591) | 0.2262 | 0.068 | 4 |
LiCr2(PO4)3 (mp-31667) | 0.2037 | 0.028 | 4 |
MoO2 (mvc-6944) | 0.7079 | 0.387 | 2 |
Li2MgCr3(SO4)6 (mp-774307) | 0.3154 | 0.279 | 5 |
Li9Nb10Cr6(PO4)24 (mp-851292) | 0.3091 | 0.030 | 5 |
Li2MnV(PO4)3 (mp-770055) | 0.3439 | 0.030 | 5 |
LiMgCr3(SO4)6 (mp-769554) | 0.3529 | 0.229 | 5 |
Li2MnV(PO4)3 (mp-770169) | 0.3103 | 0.026 | 5 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.4648 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4397 | 0.003 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.3704 | 0.114 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.4643 | 0.041 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4721 | 0.015 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7171 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-7.3054 eV |
Corrected Energy-594.5089 eV
-594.5089 eV = -525.9909 eV (uncorrected energy) - 34.8080 eV (MP Advanced Correction) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)