Final Magnetic Moment13.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.313 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.028 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + CoPO4 + FePO4 |
Band Gap0.222 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <1 0 0> | 173.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 176.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 209.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 143.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 143.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 104.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 173.3 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 177.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 176.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 176.2 |
BN (mp-984) | <1 0 0> | <0 1 1> | 155.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 260.0 |
Al (mp-134) | <1 1 0> | <1 0 1> | 209.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 234.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 293.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 176.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 234.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 234.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 209.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 176.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 176.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 143.4 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 104.8 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 293.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 293.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 234.9 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 58.7 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 209.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 234.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 293.6 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 260.0 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 1> | 155.0 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 104.8 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 293.6 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 293.6 |
Au (mp-81) | <1 1 0> | <1 0 0> | 173.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 117.5 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 293.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 293.6 |
C (mp-48) | <1 0 0> | <0 1 1> | 155.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 234.9 |
SiC (mp-11714) | <1 0 0> | <0 1 1> | 155.0 |
MoSe2 (mp-1634) | <1 1 1> | <1 1 1> | 177.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 234.9 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 293.6 |
WSe2 (mp-1821) | <1 1 1> | <1 1 1> | 177.6 |
Au (mp-81) | <1 0 0> | <1 0 1> | 104.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 176.2 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 209.6 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 293.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnCrO4 (mp-780641) | 0.2843 | 0.104 | 3 |
FePO4 (mp-25001) | 0.2845 | 0.024 | 3 |
V3(P2O7)2 (mp-32416) | 0.3637 | 0.033 | 3 |
Co2P3O10 (mp-25658) | 0.3593 | 0.123 | 3 |
Ni2P3O10 (mp-25610) | 0.2992 | 0.052 | 3 |
MnFe3(PO4)4 (mp-767822) | 0.0885 | 0.449 | 4 |
FeCo3(PO4)4 (mp-772363) | 0.0915 | 0.045 | 4 |
MnFe3(PO4)4 (mp-767591) | 0.0880 | 0.019 | 4 |
MnFe3(PO4)4 (mp-773269) | 0.0796 | 0.020 | 4 |
MnFe(PO4)2 (mp-767833) | 0.0704 | 0.016 | 4 |
CrO2 (mvc-11581) | 0.7266 | 0.166 | 2 |
Cr5O12 (mp-19575) | 0.7227 | 0.142 | 2 |
VO2 (mvc-6918) | 0.7054 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6867 | 0.281 | 2 |
MnFeCo(PO4)3 (mp-764410) | 0.0945 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.0424 | 0.029 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.0767 | 0.300 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.1174 | 0.333 | 5 |
MnFeCo(PO4)3 (mp-764739) | 0.1016 | 0.025 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.7069 | 0.080 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5614 | 0.257 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6890 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6963 | 0.331 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.7191 | 0.015 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7141 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV Co: 3.32 eV |
PseudopotentialsVASP PAW: Mn_pv Fe_pv Co P O |
Final Energy/Atom-7.0712 eV |
Corrected Energy-567.9892 eV
-567.9892 eV = -509.1278 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 25.1514 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)