Final Magnetic Moment8.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.262 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi2P2O7 + MnPO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 316.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 63.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 175.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 316.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 316.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 190.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 253.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 316.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 190.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 253.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 175.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 190.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 316.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 190.1 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 316.8 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 253.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 63.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 190.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 190.1 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 63.4 |
C (mp-48) | <0 0 1> | <0 0 1> | 63.4 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 253.4 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 190.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 190.1 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 175.6 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 253.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 316.8 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 316.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 190.1 |
C (mp-66) | <1 1 1> | <1 0 0> | 175.6 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 316.8 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 253.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 63.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 190.1 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 63.4 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 316.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 63.4 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 253.4 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 190.1 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 63.4 |
Au (mp-81) | <1 0 0> | <0 0 1> | 316.8 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 190.1 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 253.4 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 253.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 190.1 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 316.8 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 253.4 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 175.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.2050 | 0.050 | 3 |
VPO4 (mp-861584) | 0.1347 | 0.076 | 3 |
FePO4 (mp-773675) | 0.2784 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1423 | 0.077 | 3 |
TiPO4 (mp-25435) | 0.3977 | 0.087 | 3 |
FeCu(PO4)2 (mp-771351) | 0.0952 | 0.086 | 4 |
V5Cr(PO4)6 (mp-770858) | 0.1016 | 0.063 | 4 |
Ti5Cr(PO4)6 (mp-776640) | 0.1178 | 0.084 | 4 |
V2Ni(PO4)3 (mp-774099) | 0.0841 | 0.029 | 4 |
Mn2Co(PO4)3 (mp-761760) | 0.0531 | 0.089 | 4 |
VO2 (mvc-6918) | 0.6857 | 0.094 | 2 |
MoO2 (mvc-6944) | 0.6392 | 0.281 | 2 |
Mn3FeNi2(PO4)6 (mp-771527) | 0.1056 | 0.026 | 5 |
Mn3Co2Sn(PO4)6 (mp-997524) | 0.1119 | 0.095 | 5 |
Mn3Fe2Co(PO4)6 (mp-762278) | 0.1100 | 0.107 | 5 |
Mn3VNi2(PO4)6 (mp-868582) | 0.1118 | 0.047 | 5 |
MnFe3Ni2(PO4)6 (mp-781284) | 0.1174 | 0.026 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5729 | 0.065 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5820 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3585 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5307 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.6061 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Mn_pv Ni_pv P O |
Final Energy/Atom-7.0265 eV |
Corrected Energy-280.8592 eV
-280.8592 eV = -252.9528 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 11.0514 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)