Final Magnetic Moment6.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.670 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3V2(PO4)3 + VPO4 |
Band Gap2.200 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 297.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 223.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 148.7 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 184.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 223.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 297.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 223.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 297.3 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 129.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 223.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 297.3 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 113.6 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 141.6 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 259.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 259.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 223.0 |
BN (mp-984) | <1 0 1> | <1 0 1> | 140.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 238.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 297.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 238.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 129.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 227.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 297.3 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 227.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 0> | 227.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 297.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 223.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 -1> | 141.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 238.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 297.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 148.7 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 148.7 |
InP (mp-20351) | <1 0 0> | <0 1 -1> | 141.6 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 223.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 -1> | 141.6 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 1> | 259.4 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 1> | 259.4 |
PbS (mp-21276) | <1 0 0> | <0 1 -1> | 141.6 |
Au (mp-81) | <1 0 0> | <0 1 1> | 259.4 |
C (mp-48) | <1 1 1> | <0 0 1> | 297.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 148.7 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 259.4 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 -1> | 184.9 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 129.7 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 1> | 259.4 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 1> | 259.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 223.0 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 1> | 259.4 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 223.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2PO5 (mp-770547) | 0.5551 | 0.000 | 3 |
Ni7(PO4)6 (mp-771985) | 0.5745 | 0.055 | 3 |
Co3(AsO4)2 (mp-25740) | 0.5800 | 0.003 | 3 |
Zn3(AsO4)2 (mp-16834) | 0.5871 | 0.000 | 3 |
Co3(PO4)2 (mp-608109) | 0.5584 | 0.000 | 3 |
Li3Fe3(PO4)4 (mp-763894) | 0.1188 | 0.043 | 4 |
Li3Fe3(PO4)4 (mp-31842) | 0.2651 | 0.011 | 4 |
Li3Mn3(PO4)4 (mp-32029) | 0.2657 | 0.003 | 4 |
Li3Cr3(PO4)4 (mp-779385) | 0.2070 | 0.094 | 4 |
Li3Mn3(PO4)4 (mp-585338) | 0.2484 | 0.000 | 4 |
LiMnPO4F (mp-762683) | 0.7467 | 0.020 | 5 |
FeCoPO4F (mp-705338) | 0.7148 | 0.015 | 5 |
LiCrPO4F (mp-762791) | 0.5769 | 0.072 | 5 |
LiPWO4F (mp-25652) | 0.7307 | 0.057 | 5 |
Y4Ti13Si2(SbO14)2 (mvc-9261) | 0.7307 | 0.392 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.1903 eV |
Corrected Energy-609.6932 eV
-609.6932 eV = -560.8452 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 15.1380 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)