Final Magnetic Moment12.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.551 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2PO5 + LiVPO4 + V4P3 + VPO4 |
Band Gap2.119 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI42d [122] |
HallI 4 2bw |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 233.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 261.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 233.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 279.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 186.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 279.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 186.5 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 233.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 233.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 138.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 139.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 139.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 261.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 233.1 |
Al (mp-134) | <1 1 0> | <1 0 1> | 138.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 139.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 46.6 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 186.5 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 233.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 93.3 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 233.1 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 233.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 233.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 279.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 233.1 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 233.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 186.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 279.8 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 233.1 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 261.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 46.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 186.5 |
Ni (mp-23) | <1 1 0> | <1 0 1> | 138.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 326.4 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 233.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 233.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 186.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 233.1 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 326.4 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 186.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 326.4 |
Si (mp-149) | <1 0 0> | <0 0 1> | 233.1 |
Si (mp-149) | <1 1 1> | <1 0 0> | 261.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 233.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 186.5 |
C (mp-48) | <1 0 0> | <0 0 1> | 233.1 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 139.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 233.1 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 279.8 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 233.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co3(AsO4)2 (mp-863909) | 0.5825 | 0.000 | 3 |
Ni2PO5 (mp-775542) | 0.6300 | 0.026 | 3 |
Mg3(AsO4)2 (mp-758196) | 0.5806 | 0.038 | 3 |
Mn2PO5 (mp-770114) | 0.6010 | 0.029 | 3 |
V2PO5 (mp-19007) | 0.6652 | 0.000 | 3 |
LiMg4V3O12 (mp-565332) | 0.4620 | 0.002 | 4 |
LiCr4(PO4)3 (mp-775232) | 0.1060 | 0.285 | 4 |
LiNi4(PO4)3 (mp-32332) | 0.1465 | 0.075 | 4 |
LiMn4(PO4)3 (mp-585189) | 0.1921 | 0.047 | 4 |
LiFe4(PO4)3 (mp-762543) | 0.1238 | 0.040 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.7009 | 0.022 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.6868 | 0.131 | 5 |
Li7Fe7P6(O8F)3 (mp-997551) | 0.7229 | 0.219 | 5 |
Li3MnV(PO4)3 (mp-778558) | 0.7233 | 0.090 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.4854 eV |
Corrected Energy-329.5048 eV
Uncorrected energy = -299.4168 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.700 eV/atom x 8.0 atoms) = -13.6000 eV
Corrected energy = -329.5048 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)