Final Magnetic Moment6.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.807 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn(CO3)2 + MnO2 + CO2 |
Band Gap0.719 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 204.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 218.0 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 68.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 159.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 159.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 265.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 274.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 223.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 223.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 95.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 127.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 275.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 351.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 159.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 223.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 255.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 191.5 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 68.2 |
GaN (mp-804) | <1 1 1> | <1 -1 1> | 247.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 218.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 204.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 95.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 1> | 165.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 275.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 274.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 267.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 274.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 255.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 127.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 321.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 287.3 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 219.9 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 272.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 95.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 130.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 95.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 265.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 274.9 |
CdS (mp-672) | <0 0 1> | <1 -1 1> | 247.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 95.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 255.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 136.3 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 305.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 255.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.4 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 164.9 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 321.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 95.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 287.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 159.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2(CO3)3 (mp-762590) | 0.6875 | 0.280 | 3 |
Co2(CO3)3 (mp-997509) | 0.6649 | 0.189 | 3 |
Li3Mn2(CO3)4 (mp-764946) | 0.5454 | 0.056 | 4 |
LiV2(CO3)4 (mp-763681) | 0.3711 | 0.079 | 4 |
LiMn(CO3)2 (mp-763549) | 0.5072 | 0.281 | 4 |
LiFe2(CO3)4 (mp-763524) | 0.5670 | 0.097 | 4 |
LiFe2(CO3)4 (mp-763371) | 0.4828 | 0.086 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv C O |
Final Energy/Atom-7.3187 eV |
Corrected Energy-150.8454 eV
-150.8454 eV = -139.0562 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)