Final Magnetic Moment0.096 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.541 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.124 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiV2(PO4)3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 196.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 107.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 343.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 133.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 245.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 175.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 266.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 343.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 196.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 147.3 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 107.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 245.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 343.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 196.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 343.7 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 215.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 110.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 221.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 294.6 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 175.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 245.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 196.4 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 215.0 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 133.1 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 221.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 343.7 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 98.2 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 107.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 343.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 147.3 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 294.6 |
C (mp-66) | <1 1 0> | <1 0 -1> | 107.5 |
PbS (mp-21276) | <1 0 0> | <1 0 -1> | 107.5 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 245.5 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 343.7 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 343.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 196.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 343.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 196.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 221.2 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 266.3 |
LaF3 (mp-905) | <1 1 1> | <1 0 0> | 98.2 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 196.4 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 343.7 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 245.5 |
SiC (mp-11714) | <0 0 1> | <1 0 1> | 133.1 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 245.5 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 107.5 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 343.7 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 196.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr(PO3)2 (mp-772684) | 0.5698 | 0.173 | 3 |
Fe4(PO4)3 (mp-31780) | 0.4931 | 0.007 | 3 |
P4W3O14 (mvc-1031) | 0.5868 | 0.315 | 3 |
Cr4(PO4)3 (mp-31658) | 0.4460 | 0.100 | 3 |
Cu(PO3)2 (mp-558839) | 0.5799 | 0.000 | 3 |
Li2Fe2(SO4)3 (mp-778400) | 0.4842 | 0.280 | 4 |
Li2Ni2(SO4)3 (mp-770331) | 0.4816 | 0.077 | 4 |
LiFe2(SO4)3 (mp-770180) | 0.4733 | 0.218 | 4 |
LiBi2(PO4)3 (mp-585241) | 0.4367 | 0.062 | 4 |
LiBi2(PO4)3 (mp-26301) | 0.4865 | 0.078 | 4 |
Li2ZrFe(PO4)3 (mp-767488) | 0.5706 | 0.170 | 5 |
KLiTi2(PO5)2 (mp-774482) | 0.5480 | 0.027 | 5 |
Li3MnV(PO4)3 (mp-778890) | 0.5499 | 0.068 | 5 |
Li2MnV(PO4)3 (mp-770135) | 0.5625 | 0.216 | 5 |
KLiTi2(PO5)2 (mp-776444) | 0.5219 | 0.015 | 5 |
Li4Mn2CrNi3(PO4)6 (mp-775171) | 0.6219 | 0.085 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5540 | 0.080 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5721 | 0.015 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6254 | 0.081 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6122 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.2017 eV |
Corrected Energy-282.8426 eV
-282.8426 eV = -259.2596 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)