Final Magnetic Moment7.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.831 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Ti3VO8 + LiVO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 -1> | 214.8 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 160.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 159.5 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 204.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 322.7 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 179.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 210.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 300.2 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 138.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 270.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 280.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 160.6 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 -1> | 227.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 153.2 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 119.6 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 153.2 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 230.5 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 153.2 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 138.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 179.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 200.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 270.2 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 322.7 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 160.6 |
KCl (mp-23193) | <1 1 0> | <1 -1 -1> | 227.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 160.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 214.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 330.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 280.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 321.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 270.2 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 138.3 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 230.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 270.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 280.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 149.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 212.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 280.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 306.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 150.1 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 200.2 |
LiF (mp-1138) | <1 0 0> | <1 -1 1> | 149.0 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 119.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 319.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 -1> | 161.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 160.1 |
YVO4 (mp-19133) | <1 0 1> | <0 1 -1> | 214.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 200.2 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 92.2 |
YVO4 (mp-19133) | <1 1 0> | <0 1 -1> | 322.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2(NiO2)3 (mp-762391) | 0.2157 | 0.039 | 3 |
Li2V3O6 (mp-762271) | 0.1849 | 0.050 | 3 |
Li3V7O12 (mp-762285) | 0.1931 | 0.078 | 3 |
Li2Ti3O6 (mp-760539) | 0.1922 | 0.064 | 3 |
Li2(FeO2)3 (mp-763691) | 0.1953 | 0.283 | 3 |
Li4Cr3(FeO4)3 (mp-780090) | 0.1338 | 1.279 | 4 |
Li2MnCr2O6 (mp-850919) | 0.1154 | 0.056 | 4 |
Li2Cr2FeO6 (mp-782636) | 0.1203 | 0.804 | 4 |
Li4V3Cr3O12 (mp-850080) | 0.1444 | 0.053 | 4 |
Li2Ti(FeO3)2 (mp-762684) | 0.1246 | 0.246 | 4 |
Ni6O7 (mp-767815) | 0.2605 | 0.047 | 2 |
V6C5 (mp-28731) | 0.2097 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.2638 | 0.064 | 2 |
Nb6C5 (mp-2760) | 0.2358 | 0.000 | 2 |
Ni6Cl7 (mp-1022720) | 0.2575 | 0.376 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4589 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-7.5801 eV |
Corrected Energy-180.2365 eV
-180.2365 eV = -166.7630 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 5.0460 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)