Final Magnetic Moment15.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.341 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFePO4 + VPO5 + Ni2P2O7 |
Band Gap1.229 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 320.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 320.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 320.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 192.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 192.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 256.0 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 320.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 192.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 176.0 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 192.0 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 320.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 320.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 256.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 320.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 256.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 256.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 192.0 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.0 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 192.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 256.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 256.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 320.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 192.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 256.0 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 256.0 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 256.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 192.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 192.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 176.0 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 256.0 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 320.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 320.0 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 192.0 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 320.0 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 256.0 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 176.0 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 192.0 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 64.0 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 320.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe7(PO5)4 (mp-761434) | 0.4145 | 0.768 | 3 |
MnPO4 (mp-773411) | 0.3012 | 0.344 | 3 |
VPO4 (mp-861584) | 0.2264 | 0.079 | 3 |
FePO4 (mp-773675) | 0.3370 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.2303 | 0.077 | 3 |
TiNi(PO4)2 (mp-761309) | 0.1048 | 0.012 | 4 |
TiFe5(PO4)6 (mp-773598) | 0.1254 | 0.322 | 4 |
TiNi5(PO4)6 (mp-773434) | 0.1115 | 0.217 | 4 |
VFe5(PO4)6 (mp-782634) | 0.1216 | 0.028 | 4 |
VNi5(PO4)6 (mp-771180) | 0.0729 | 0.080 | 4 |
VO2 (mvc-6918) | 0.7246 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6912 | 0.281 | 2 |
Ti3Co2Ni(PO4)6 (mp-850089) | 0.1130 | 0.064 | 5 |
Ti3CoNi2(PO4)6 (mp-776907) | 0.0972 | 0.043 | 5 |
Ti3CuNi2(PO4)6 (mp-776876) | 0.0969 | 0.034 | 5 |
TiMn2Ni3(PO4)6 (mp-776680) | 0.0855 | 0.086 | 5 |
Ti3FeNi2(PO4)6 (mp-778326) | 0.1044 | 0.019 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5407 | 0.068 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5227 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5163 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3385 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4636 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV Ni: 6.2 eV |
PseudopotentialsVASP PAW: V_pv Fe_pv Ni_pv P O |
Final Energy/Atom-6.9583 eV |
Corrected Energy-281.5610 eV
-281.5610 eV = -250.4970 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 14.2090 eV (MP Advanced Correction)
|