Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.933 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVO2 + Li2Ti3VO8 + Li2TiO3 + V |
Band Gap0.270 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 236.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 162.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 228.5 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 69.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 278.0 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 208.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 315.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 177.1 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 76.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 270.4 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 69.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 236.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 0> | 309.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 225.4 |
CdS (mp-672) | <1 0 1> | <1 -1 0> | 232.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 163.6 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 208.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 270.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 304.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 208.5 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 278.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 54.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 162.0 |
BN (mp-984) | <1 1 0> | <1 1 1> | 69.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 135.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 218.2 |
Al (mp-134) | <1 1 1> | <1 -1 0> | 309.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 176.7 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 270.0 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 270.0 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 69.5 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 278.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 242.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 323.9 |
C (mp-66) | <1 1 0> | <0 1 1> | 176.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 315.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 270.4 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 323.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 270.0 |
Mg (mp-153) | <1 0 1> | <1 -1 1> | 267.8 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 323.9 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 162.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.4 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 309.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 225.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 208.5 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 135.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 180.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 323.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 225.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe5O12 (mp-762602) | 0.1835 | 0.058 | 3 |
Li5Cr5O12 (mp-762528) | 0.1999 | 0.102 | 3 |
Li3V7O12 (mp-762285) | 0.1523 | 0.082 | 3 |
Li7(NiO2)10 (mp-767858) | 0.2461 | 0.032 | 3 |
Li5V5O12 (mp-762939) | 0.1836 | 0.087 | 3 |
Li2Mn2NiO6 (mp-762672) | 0.1528 | 0.067 | 4 |
Li3Cr2Fe5O12 (mp-780009) | 0.1814 | 0.967 | 4 |
Li2Fe2NiO6 (mp-762754) | 0.1518 | 0.121 | 4 |
Li2V2FeO6 (mp-762806) | 0.1304 | 0.116 | 4 |
Li2V2CrO6 (mp-849330) | 0.1817 | 0.063 | 4 |
Ni6O7 (mp-767815) | 0.3011 | 0.057 | 2 |
Ni5O6 (mp-782702) | 0.3174 | 0.041 | 2 |
V6C5 (mp-28731) | 0.3234 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.3542 | 0.063 | 2 |
Ni6Cl7 (mp-1022720) | 0.3452 | 0.376 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4223 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-7.7044 eV |
Corrected Energy-271.9338 eV
-271.9338 eV = -254.2465 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 5.0460 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)