Final Magnetic Moment2.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.543 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO5 + VO2 |
Band Gap1.165 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 51.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 207.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 155.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 125.7 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 259.4 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 238.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 175.5 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 281.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 197.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 207.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 125.7 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 251.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 225.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 238.4 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 238.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 273.5 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 205.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 49.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 189.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 197.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 207.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 112.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 197.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 148.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 234.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 -1> | 273.5 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 125.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 155.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 259.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 51.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 207.5 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 273.5 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 337.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 225.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 238.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 238.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 251.3 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 314.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 189.0 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 216.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 292.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 135.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 197.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 197.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 162.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 207.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 197.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 311.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 188.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-673151) | 0.5598 | 0.038 | 3 |
Cu2PO4 (mp-17281) | 0.5339 | 0.000 | 3 |
Ga3PO7 (mp-3107) | 0.5303 | 0.016 | 3 |
Fe3PO7 (mp-18775) | 0.5203 | 0.052 | 3 |
Cr4(PO4)3 (mp-774538) | 0.5827 | 0.041 | 3 |
LiCu4(PO4)3 (mp-673145) | 0.5791 | 0.050 | 4 |
Li3Fe3(PO4)4 (mp-31797) | 0.5737 | 0.051 | 4 |
LiVPO5 (mp-777072) | 0.5534 | 0.069 | 4 |
ZnSnAs2O7 (mvc-7618) | 0.5484 | 0.144 | 4 |
MgAlPO5 (mp-555548) | 0.5804 | 0.004 | 4 |
CrN2 (mp-1016069) | 0.7090 | 0.474 | 2 |
CrN2 (mp-1096899) | 0.7056 | 0.474 | 2 |
LiFe3SiPO8 (mp-743761) | 0.6170 | 0.105 | 5 |
NaCaMgAl(SiO3)4 (mp-720244) | 0.6862 | 0.312 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.2563 eV |
Corrected Energy-176.1996 eV
-176.1996 eV = -159.6395 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)