Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.631 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4F + LiF |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFmm2 [42] |
HallF 2 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 248.6 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 248.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 94.4 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 280.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 280.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 280.8 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 280.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 165.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 165.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 280.8 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 251.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 82.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 132.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 283.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 82.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 82.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 283.2 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 132.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 82.9 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 280.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 93.6 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 248.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 165.7 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 1> | 125.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 280.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 1> | 125.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 82.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 280.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 132.9 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 280.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 93.6 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 132.9 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 280.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 165.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 165.7 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 248.6 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 283.2 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 165.7 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 280.8 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 93.6 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 1> | 250.0 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 165.7 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 0> | 93.6 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 248.6 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 280.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 165.7 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 280.8 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 248.6 |
WSe2 (mp-1821) | <1 0 0> | <0 1 1> | 250.0 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 165.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na5Mn2O8 (mp-849237) | 0.7495 | 0.083 | 3 |
Ca3SiO5 (mp-641754) | 0.6979 | 0.020 | 3 |
Ca3SiO5 (mp-27917) | 0.6541 | 0.062 | 3 |
Na8Fe2O7 (mp-555787) | 0.7292 | 0.000 | 3 |
Na8V2O7 (mp-778356) | 0.6975 | 0.060 | 3 |
Li3V(PO4)2 (mp-773542) | 0.7237 | 0.065 | 4 |
VAg2O3F (mp-704944) | 0.6223 | 0.015 | 4 |
Na3LaV2O8 (mp-579223) | 0.7444 | 0.005 | 4 |
CaMn(GeO3)2 (mvc-8897) | 0.6891 | 0.028 | 4 |
CaSb2P2O9 (mvc-9691) | 0.7117 | 0.072 | 4 |
Na3V2P2O8F3 (mp-694937) | 0.6072 | 0.000 | 5 |
Li3Mn2P2O8F3 (mp-763737) | 0.5989 | 0.071 | 5 |
Li3V2P2O8F3 (mp-763720) | 0.6827 | 0.060 | 5 |
Na3Ti2P2O10F (mp-41191) | 0.6402 | 0.005 | 5 |
Na3Fe2P2O8F3 (mp-581813) | 0.5116 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O F |
Final Energy/Atom-6.5060 eV |
Corrected Energy-252.1776 eV
-252.1776 eV = -234.2176 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|