Final Magnetic Moment12.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.668 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.053 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3PO4 + Li3Cr2(PO4)3 + LiCrPO4F + Cr2O3 |
Band Gap1.905 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 178.6 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 178.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 206.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 275.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 192.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 -1> | 288.3 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 192.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 275.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 -1> | 222.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 275.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 275.1 |
TiO2 (mp-2657) | <0 0 1> | <0 1 -1> | 192.2 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 197.3 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 98.6 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 288.3 |
C (mp-66) | <1 1 0> | <0 1 -1> | 288.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 206.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 275.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 275.1 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 178.6 |
LaF3 (mp-905) | <1 0 1> | <1 0 -1> | 222.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 295.9 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 288.3 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 275.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 222.1 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 98.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 68.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.1 |
PbSe (mp-2201) | <1 0 0> | <0 1 -1> | 192.2 |
Al (mp-134) | <1 1 1> | <0 1 -1> | 288.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 275.1 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 -1> | 192.2 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 178.6 |
Au (mp-81) | <1 1 0> | <0 0 1> | 275.1 |
CdSe (mp-2691) | <1 0 0> | <0 1 -1> | 192.2 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 275.1 |
WS2 (mp-224) | <1 0 0> | <1 0 -1> | 222.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 206.3 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 -1> | 288.3 |
MgF2 (mp-1249) | <1 0 0> | <0 1 -1> | 288.3 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 295.9 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 295.9 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 275.1 |
MgF2 (mp-1249) | <0 0 1> | <0 1 1> | 197.3 |
ZnO (mp-2133) | <0 0 1> | <1 1 1> | 178.6 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 -1> | 288.3 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 0 1> | 275.1 |
GaSb (mp-1156) | <1 0 0> | <0 1 -1> | 192.2 |
ZnTe (mp-2176) | <1 0 0> | <0 1 -1> | 192.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4CoO4 (mp-763322) | 0.7365 | 0.168 | 3 |
Li3Mn(PO4)2 (mp-863896) | 0.7210 | 0.018 | 4 |
Ca2AlSnO5 (mvc-5761) | 0.6590 | 0.146 | 4 |
Li3V(PO4)2 (mp-540311) | 0.7166 | 0.026 | 4 |
Li3Fe(PO4)2 (mp-540396) | 0.7183 | 0.170 | 4 |
Ca2AlMoO5 (mvc-5371) | 0.6451 | 0.102 | 4 |
Li2CoPO4F (mp-25488) | 0.6051 | 0.054 | 5 |
Li2MnPO4F (mp-25562) | 0.5290 | 0.045 | 5 |
Li2VPO4F (mp-25630) | 0.5260 | 0.036 | 5 |
Li2FePO4F (mp-25688) | 0.5422 | 0.040 | 5 |
Li2NiPO4F (mp-25605) | 0.5450 | 0.030 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O F |
Final Energy/Atom-6.5506 eV |
Corrected Energy-471.5234 eV
-471.5234 eV = -438.8912 eV (uncorrected energy) - 24.5801 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)