Final Magnetic Moment54.415 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.764 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4Mn5O12 + MnO2 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 235.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 235.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 140.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 117.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 176.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 159.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 140.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 235.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 140.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 294.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 117.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 294.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 117.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 58.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 140.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 294.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 58.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 117.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 176.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 294.4 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 159.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 159.0 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 140.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 140.0 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 294.4 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 140.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 235.5 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 58.9 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 176.6 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 -1> | 144.4 |
Au (mp-81) | <1 1 0> | <0 0 1> | 294.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 58.9 |
C (mp-48) | <0 0 1> | <0 0 1> | 294.4 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 176.6 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 176.6 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 176.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 117.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 58.9 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 117.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 140.0 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 159.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 294.4 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 294.4 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 176.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 176.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 176.6 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 235.5 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 140.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 294.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 159.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li10Mn21O48 (mp-698592) | 0.3672 | 0.051 | 3 |
Mn6Zn3O16 (mp-774014) | 0.2623 | 0.064 | 3 |
Li2Mn5O12 (mp-763571) | 0.1592 | 0.084 | 3 |
Li2Mn15O32 (mp-34891) | 0.2962 | 0.105 | 3 |
Li2Mn15O32 (mp-698551) | 0.2919 | 0.105 | 3 |
Zn3Cu10(TeO6)6 (mvc-15145) | 0.7017 | 0.059 | 4 |
CoO2 (mvc-12170) | 0.3186 | 0.104 | 2 |
FeO2 (mvc-15135) | 0.3668 | 0.277 | 2 |
NiO2 (mvc-13696) | 0.3536 | 0.322 | 2 |
MnO2 (mvc-10183) | 0.3255 | 0.152 | 2 |
NiO2 (mvc-10289) | 0.3416 | 0.284 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O |
Final Energy/Atom-6.6607 eV |
Corrected Energy-476.2888 eV
-476.2888 eV = -419.6227 eV (uncorrected energy) - 28.5745 eV (MP Advanced Correction) - 28.0916 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)