Final Magnetic Moment0.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.499 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaLi2PO4 + Na4VP2O9 + Na2V3O7 |
Band Gap2.391 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 222.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 311.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 299.9 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 266.9 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 174.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 300.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 311.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 150.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 225.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 299.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 222.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 225.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 262.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 222.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 311.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 225.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 222.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 311.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 311.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 222.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 222.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 225.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 311.3 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 87.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 75.2 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 100.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 262.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 300.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 177.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 222.4 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 262.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 300.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 177.9 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 218.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 -1> | 100.0 |
Al (mp-134) | <1 1 1> | <0 1 0> | 222.4 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 222.4 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 311.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 222.9 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 177.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 311.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 311.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 299.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 75.2 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 311.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 311.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 133.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 0> | 222.4 |
GdScO3 (mp-5690) | <1 1 1> | <1 1 -1> | 218.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na14Al4O13 (mp-31008) | 0.5783 | 0.000 | 3 |
Mg2SiO4 (mp-675215) | 0.5604 | 0.195 | 3 |
Na17Al5O16 (mp-559916) | 0.5472 | 0.002 | 3 |
Na3MoN3 (mp-541291) | 0.5547 | 0.000 | 3 |
Na7Al3O8 (mp-556168) | 0.5481 | 0.000 | 3 |
Na2VPO6 (mp-764095) | 0.5053 | 0.020 | 4 |
Li3Sb2(PO4)3 (mp-759227) | 0.4965 | 0.065 | 4 |
Li2Fe2B2O7 (mp-779057) | 0.4839 | 0.073 | 4 |
LiCrPO4 (mp-772700) | 0.4797 | 0.097 | 4 |
LiCoPO4 (mp-761732) | 0.4596 | 0.070 | 4 |
Li4Mn5Co(PO4)6 (mp-765461) | 0.5766 | 0.069 | 5 |
Li4Mn5Sn(PO4)6 (mp-853140) | 0.5835 | 0.078 | 5 |
Li2Mn2Fe(PO4)3 (mp-776051) | 0.5733 | 0.094 | 5 |
Li2Mn2Co(PO4)3 (mp-763122) | 0.5601 | 0.086 | 5 |
Sr2AlGaFe2O7 (mvc-13325) | 0.6091 | 0.120 | 5 |
Li4Mn3CuNi2(PO4)6 (mp-775323) | 0.6225 | 0.080 | 6 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.5897 | 0.095 | 6 |
Li4Cr2Ni3Sn(PO4)6 (mp-778614) | 0.6180 | 0.183 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.5425 | 0.102 | 6 |
Li4Mn2Fe3Sb(PO4)6 (mp-776752) | 0.6160 | 3.420 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv V_pv P O |
Final Energy/Atom-6.3917 eV |
Corrected Energy-304.8196 eV
-304.8196 eV = -281.2366 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)