Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.455 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.077 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa5Li(PO4)2 + LiMnBO3 + NaBO2 + MnO |
Band Gap2.432 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 200.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 182.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 305.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 247.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 250.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 328.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 182.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 328.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 255.2 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 305.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 109.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 328.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 182.3 |
BN (mp-984) | <0 0 1> | <0 1 1> | 186.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 250.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 300.8 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 247.8 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 229.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 328.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 247.8 |
LiTaO3 (mp-3666) | <1 1 1> | <0 1 0> | 250.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 255.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 255.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 328.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 182.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 145.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 72.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 72.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 1> | 229.1 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 229.1 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 250.6 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 328.2 |
TbScO3 (mp-31119) | <1 1 0> | <1 1 1> | 182.7 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 182.7 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 309.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 255.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 182.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 255.2 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 1> | 229.1 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 131.3 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 262.5 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 262.5 |
NdGaO3 (mp-3196) | <1 1 0> | <1 1 1> | 182.7 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 182.3 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 328.1 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 328.1 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 109.4 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 109.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 328.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeBi25O39 (mp-698573) | 0.7117 | 0.027 | 3 |
GaBi25O39 (mp-849761) | 0.7062 | 0.021 | 3 |
FeBi25O39 (mp-761437) | 0.7086 | 0.025 | 3 |
Na2Ti2O5 (mp-779729) | 0.7289 | 0.035 | 3 |
Zn(Bi19O30)2 (mp-773918) | 0.6574 | 0.029 | 3 |
LiMnPO4 (mp-761562) | 0.6715 | 0.078 | 4 |
LiFePO4 (mp-762593) | 0.6679 | 0.844 | 4 |
Li3B5(HO5)2 (mp-707105) | 0.6705 | 0.000 | 4 |
NaLiCO3 (mp-559533) | 0.6604 | 0.000 | 4 |
NaLiCO3 (mp-556783) | 0.6454 | 0.000 | 4 |
Bi19O30 (mp-773884) | 0.6942 | 0.050 | 2 |
Li3NiPCO7 (mp-861721) | 0.4938 | 0.121 | 5 |
Li3CoPCO7 (mp-767342) | 0.4962 | 0.153 | 5 |
Li5Mn2P2(CO7)2 (mp-770047) | 0.4820 | 0.036 | 5 |
Li3CuAsCO7 (mp-768589) | 0.4818 | 0.067 | 5 |
Na3BSbAsO7 (mp-770738) | 0.4851 | 0.055 | 5 |
Li12Cr3FeP4(CO7)4 (mp-767736) | 0.5920 | 1.139 | 6 |
Li12Mn3CrP4(CO7)4 (mp-767734) | 0.5489 | 0.056 | 6 |
Li6MnCrP2(CO7)2 (mp-767287) | 0.5477 | 0.062 | 6 |
NaLi5Mn2P2(CO7)2 (mp-773931) | 0.5944 | 0.206 | 6 |
NaLi5Mn2P2(CO7)2 (mp-773772) | 0.5894 | 0.047 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv B P O |
Final Energy/Atom-6.3940 eV |
Corrected Energy-192.2249 eV
-192.2249 eV = -179.0312 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)